Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Plaskolite West Optix® CP - 51 KC General Purpose Acrylic Resin

Category Polymer , Thermoplastic , Acrylic (PMMA) , Acrylic, General Purpose, Molded , Acrylic, Optical Grade, Molded
Manufacturer Plaskolite West, Inc.
Trade Name Optix®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plaskolite West Optix® CP - 51 KC General Purpose Acrylic Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are available.Information provided by Plaskolite West, Inc.
Physical Properties Metric English Comments
Density 1.19 g/cc
0.0430 lb/in³
ASTM D-792
Linear Mold Shrinkage 0.0020 - 0.0060 cm/cm
0.0020 - 0.0060 in/in
ASTM D-955
Melt Flow 21 g/10 min

@Load 3.80 kg,
Temperature 230 °C
21 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D-1238
Mechanical Properties Metric English Comments
Hardness, Rockwell M 80
80
ASTM D-785
Tensile Strength 53.8 MPa
7800 psi
ASTM D-638
Elongation at Break 2.6 %
2.6 %
ASTM D-638
Modulus of Elasticity 2.83 GPa
410 ksi
ASTM D-638
Flexural Strength 86.9 MPa
12600 psi
ASTM D-790
Flexural Modulus 2.98 GPa
432 ksi
ASTM D-790
Izod Impact, Notched 0.214 J/cm

@Thickness 6.35 mm
0.400 ft-lb/in

@Thickness 0.250 in
ASTM D-256
Gardner Impact 0.339 J

@Thickness 3.17 mm
0.250 ft-lb

@Thickness 0.125 in
Falling Weight; ASTM D-3029 GB
Thermal Properties Metric English Comments
CTE, linear 60.0 µm/m-°C
33.3 µin/in-°F
ASTM D-696
Deflection Temperature at 1.8 MPa (264 psi) 75.6 °C
168 °F
ASTM D-648
Vicat Softening Point 87.8 °C
190 °F
ASTM D-1525
Optical Properties Metric English Comments
Refractive Index 1.49
1.49
ASTM D-542
Haze <= 1.0 %
<= 1.0 %
ASTM D-1003
Transmission, Visible 92 %
92 %
ASTM D-1003
Users viewing this material also viewed the following: