Material Notes:
AboCast/AboCure 8006-11 is a clear dielectric casting, adhesive, and encapsulating compound. It is a 2-component, radiation-resistant, low-viscosity plasticized epoxy system. It is virtually unaffected by atmospheric conditions, soft and salt water, alkalis and diluted acids, several solvents, detergents, oils, and greases. Control of final properties by changing the AboCast/AboCure ratios: the highest rigidity, hardness, chemical and heat resistance are offered by a 100/40 ratio. Higher AboCure ratios (up to 100/100 AboCast/AboCure) yield increasing flexibility, shock and thermocycling resistance, and adhesion to problem surfaces. It has tenacious adhesion to metals, ceramics, wood, fiberglass, masonry, and most materials, to form permanent structural and dielectric bonds. Radiation resistance recommends the 8006-11 System in X-ray and other radioactive environments. Other Suggested Uses: Bonding or laminating substrates, plates lead bricks and other components in radioactive equipment; Dielectric encapsulation and potting of electronic components, especially where high thermocycling and shock resistance are needed; Shrink-free embedments and preparations of specimens for display or analytical purposes; General purpose adhesion, casting, and impregnation.
Mechanical Properties Metric English Comments
Hardness, Shore A 55
55
AboCast/AboCure ratio: 100/100 pbw
36

@Time 10.0 sec
36

@Time 0.00278 hour
AboCast/AboCure ratio: 100/100 pbw
Hardness, Shore D 18
18
AboCast/AboCure ratio: 100/100 pbw
50
50
AboCast/AboCure ratio: 100/80 pbw
78
78
AboCast/AboCure ratio: 100/40 pbw
6.0

@Time 10.0 sec
6.0

@Time 0.00278 hour
AboCast/AboCure ratio: 100/100 pbw
30

@Time 10.0 sec
30

@Time 0.00278 hour
AboCast/AboCure ratio: 100/80 pbw
Tensile Strength at Break 29.9 MPa
4330 psi
Flexural Strength 63.4 MPa
9200 psi
Compressive Strength 185 MPa
26900 psi
Izod Impact, Notched 0.294 J/cm
0.550 ft-lb/in
Processing Properties Metric English Comments
Cure Time 60.0 - 240 min

@Temperature 80.0 - 120 °C
1.00 - 4.00 hour

@Temperature 176 - 248 °F
10080 - 30240 min

@Temperature 20.0 °C
168.0 - 504.0 hour

@Temperature 68.0 °F
(1-3 weeks)
Pot Life 20 min

@Temperature 60.0 °C
20 min

@Temperature 140 °F
120 min

@Temperature 20.0 - 25.0 °C
120 min

@Temperature 68.0 - 77.0 °F
Descriptive Properties Value Comments
Hardening Time (min) 180-1440
Parts by Weight (pbw) 100
AboCast
40-100
AboCure