Samsung Cheil Industries Infino® TK-4046H PPA, Glass Filled

Category Polymer , Thermoplastic , Polyphthalamide (PPA) , Polyphthalamide (PPA), 10% Glass Fiber Reinforced
Manufacturer Samsung, Cheil Industries
Trade Name Infino®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Samsung Cheil Industries Infino® TK-4046H PPA, Glass Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Samsung Cheil Industries.
Physical Properties Metric English Comments
Specific Gravity 1.55 g/cc
1.55 g/cc
ASTM D792
Melt Flow 5.0 g/10 min

@Load 5.00 kg,
Temperature 330 °C
5.0 g/10 min

@Load 11.0 lb,
Temperature 626 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 98.1 MPa
14200 psi
5 mm/min; ASTM D638
Flexural Strength 147 MPa
21300 psi
2.8 mm/min; ASTM D790
Flexural Modulus 7.11 GPa
1030 ksi
2.8 mm/min; ASTM D790
Izod Impact, Notched 0.294 J/cm

@Thickness 3.17 mm
0.551 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 295 °C

@Thickness 6.40 mm
563 °F

@Thickness 0.252 in
ASTM D648