Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Cheng Yu Plastic BK1022 Electric Conducting Polypropylene, Injection

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer Cheng Yu Plastic Company Limited (formerly Luen Cheong Hong)
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Cheng Yu Plastic BK1022 Electric Conducting Polypropylene, Injection.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Specific Gravity 0.960 g/cc
0.960 g/cc
ASTM D792
Linear Mold Shrinkage 0.012 - 0.020 cm/cm
0.012 - 0.020 in/in
ASTM D955
Melt Index of Compound 10 - 15 g/10 min
10 - 15 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell M 100
100
ASTM D785
Tensile Strength, Yield 37.3 MPa
5400 psi
ASTM D638
Flexural Yield Strength 53.9 MPa
7820 psi
ASTM D790
Izod Impact, Notched 0.294 J/cm
0.551 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 110 °C
230 °F
ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity 1e+05
1e+05
ASTM D257