Material Notes:
Moplen HP601N is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP601N is a homopolymer typically used by customers in Glass Mat Sheet and thermoforming applications. Moplen HP601N resin meets the FDA requirements in the Code of Federal Regulations in 21 CFR 177.1520 for food contact. Features: Excellent processibility and stretchability; High mechanical propertiesApplications: Glass mat sheetInformation provided by PolyMirae Company Ltd.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 12 g/10 min

@Load 2.16 kg,
Temperature 230 °C
12 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Condition L; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 104
104
ASTM D785
Tensile Strength, Yield 34.3 MPa
4980 psi
ASTM D638
Elongation at Yield 12 %
12 %
ASTM D638
Flexural Modulus 1.67 GPa
242 ksi
ASTM D790
Izod Impact, Notched 0.294 J/cm
0.551 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 107 °C
225 °F
ASTM D648