Bapolene® 4072 Polypropylene, Injection Grade

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Bapolene®
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Bapolene® 4072 Polypropylene, Injection Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Bapolene PP4072 is a high flow, fast cycle injection molding resin. This product meets FDA standards for food contact applications.Applications: Appliances, containers, and thin-walled articles.Bapolene® and Bapolan® are registered trademarks of Bamberger Polymers, Inc. Information provided by Bamberger Polymers
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D-1505
Melt Flow 20 g/10 min
20 g/10 min
ASTM D-1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 98
98
ASTM D-785
Tensile Strength, Yield 33.1 MPa
4800 psi
ASTM D-638
Elongation at Yield 9.0 %
9.0 %
ASTM D-638
Flexural Modulus 1.28 GPa
185 ksi
ASTM D-790
Izod Impact, Notched 0.214 J/cm
0.400 ft-lb/in
ASTM D-256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 95.0 °C
203 °F
ASTM D-648
Descriptive Properties Value Comments
Process Injection Molding
Region Europe/Turkey
Bamberger Polymers Distribution
International
Bamberger Polymers Distribution
Mexico
Bamberger Polymers Distribution
US & Canada
Bamberger Polymers Distribution
Copyright © lookpolymers.com All Rights Reserved