Total PPH 3622 Polypropylene, Injection Molding Grade

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer Total Atofina
Trade Name PPH
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Total PPH 3622 Polypropylene, Injection Molding Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
General purpose injection molding and extrusion homopolymerGood Processability -- FINA 3622 is engineered for good processability in thin wall multi- cavity molds.Good Clarity -- FINA 3622 has good contact/see-through clarity, and is easily printed with silk screen or hot stamping techniques.FDA -- FINA 3622 complies with all applicable FDA regulations and may be used under those provisions for food contact applications.Recommended Applications-- FINA 3622 is recommended for the injection molding of housewares, utility boxes, and containers, as well as, general purpose extrusion.Processing -- FINA 3622 resin processes on conventional injection molding equipment with typical melt temperatures of 390- 450°F (200-232°C)Data provided by the manufacturer, Total Petrochemicals.Total Petrochemicals acquired former Fina and Atofina plastics product lines.
Physical Properties Metric English Comments
Density 0.905 g/cc
0.0327 lb/in³
ASTM D1505
Melt Flow 12 g/10 min
12 g/10 min
ASTM D1238L
Mechanical Properties Metric English Comments
Hardness, Rockwell R 103
103
ASTM D288A
Tensile Strength, Ultimate 33.1 MPa
4800 psi
ASTM D638
Elongation at Break 8.0 %
8.0 %
ASTM D638
Modulus of Elasticity 1.38 GPa
200 ksi
ASTM D638
Flexural Modulus 1.17 GPa
170 ksi
ASTM D790
Izod Impact, Notched 0.214 J/cm
0.401 ft-lb/in
ASTM D256A
Izod Impact, Unnotched 9.55 J/cm
17.9 ft-lb/in
ASTM D256A
Thermal Properties Metric English Comments
Melting Point 165 °C
329 °F
DSC
Deflection Temperature at 0.46 MPa (66 psi) 121 °C
250 °F
ASTM D648
Processing Properties Metric English Comments
Melt Temperature 200 - 232 °C
392 - 450 °F
Injection