Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Cytec Thornel® Graphite Cloth Laminate with Mil R-9299 Resin

Category Polymer , Thermoset , Carbon Fiber/Thermoset Composite , Epoxy , Epoxy/Carbon Fiber Composite
Manufacturer Cytec
Trade Name Thornel®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Cytec Thornel® Graphite Cloth Laminate with Mil R-9299 Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by the manufacturer, Amoco Performance Products, Inc.Carbon and graphite cloths, consisting entirely of flexible filaments, are produced by pyrolysis of rayon cloth at high temperatures to yield products with a high degree of purity. The cloth flexibility results from the very small filament diameter. These are fair conductors of electricity. At room temperature the volume resistivity of graphite cloth is about 40 times that of "Nichrome" wire. Graphite cloth resistance decreases with temperature, reaching half of the room temperature value at 1315°C. Cloth carbon assay is 99.9%. Filament diameter is 8.9 µm.Thornel® products were sold by Amoco and are now owned by Cytec.
Physical Properties Metric English Comments
Density 1.40 g/cc
0.0506 lb/in³
Cloth 1.42 g/cc per He measurement
Mechanical Properties Metric English Comments
Hardness, Barcol 60
60
Tensile Strength, Ultimate 103 MPa
14900 psi
Tensile Modulus 13.0 GPa
1890 ksi
Flexural Yield Strength 165 MPa
23900 psi
Flexural Modulus 13.0 GPa
1890 ksi
Compressive Yield Strength 110 MPa
16000 psi
Compressive Modulus 15.0 GPa
2180 ksi
Thermal Properties Metric English Comments
CTE, linear 11.0 µm/m-°C

@Temperature 20.0 °C
6.11 µin/in-°F

@Temperature 68.0 °F
Warp
Specific Heat Capacity 1.00 J/g-°C
0.239 BTU/lb-°F
Thermal Conductivity 10.0 W/m-K
69.4 BTU-in/hr-ft²-°F