Mechanical Properties Metric English Comments
Flexural Strength 73.0 - 76.0 MPa
10600 - 11000 psi
ASTM D790
3D Systems Accura® ClearVue™ Free (SL 7870) Stereolithography Plastic
High clarity plastic for a multitude of applicationsFeaturesClear and transparentRigid and toughGreat for headlamps, bottles and transparent assembliesExcellent humidity/moisture resistanceAll infor..
Flexural Strength 58.0 - 76.0 MPa

@Strain 5.00 %
8410 - 11000 psi

@Strain 5.00 %
ASTM D790
Arkema Group KYNAR® 1000 HD Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili..
Flexural Strength 58.0 - 76.0 MPa

@Strain 5.00 %
8410 - 11000 psi

@Strain 5.00 %
ASTM D790
Arkema Group KYNAR® 710, 710 HDP Polyvinylidene Fluoride Homopolymer- Injection Molding
Characteristics: Natural resin - translucent, off-white hemispheres. HDP indicates higher color stability. High stability in harsh thermal, chemical and ultraviolet environments. High toughness ..
Flexural Strength 58.0 - 76.0 MPa

@Strain 5.00 %
8410 - 11000 psi

@Strain 5.00 %
ASTM D790
Arkema Group KYNAR® 740 Black/Red Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion
Characteristics: Pigmented. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, abrasion resistance; high purityAppli..
Flexural Strength 58.0 - 76.0 MPa

@Strain 5.00 %
8410 - 11000 psi

@Strain 5.00 %
ASTM D790
Arkema Group KYNAR® 740 Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili..
Flexural Strength 58.0 - 76.0 MPa

@Strain 5.00 %
8410 - 11000 psi

@Strain 5.00 %
ASTM D790
Arkema Group KYNAR® 740-02 Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. Flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mecha..
Flexural Strength 58.0 - 76.0 MPa

@Strain 5.00 %
8410 - 11000 psi

@Strain 5.00 %
ASTM D790
Arkema Group KYNAR® 760 Polyvinylidene Fluoride Homopolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili..
Flexural Strength 58.0 - 76.0 MPa

@Strain 5.00 %
8410 - 11000 psi

@Strain 5.00 %
ASTM D790
Arkema Group KYNAR® 720, 720 HDP Polyvinylidene Fluoride Homopolymer- Injection Molding and Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. HDP indicates higher color stability. High stability in harsh thermal, chemical and ultraviolet environments. High toughness ..