Axiall 7765 Rigid PVC, Extrusion

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Axiall
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall 7765 Rigid PVC, Extrusion.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Georgia Gulf 7765 is a general-purpose indoor rigid PVC profile extrusion compound designed for applications requiring the following properties. 7765 carries an NSF standard 51 listing (for food zone). Impact Strength & ToughnessFlame RetardantColorabilityDimensional StabilityChemical ResistanceStiffness(High Modulus)Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.42 g/cc
1.42 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Rockwell R 93
93
ASTM D-785
Hardness, Shore D 80
80
ASTM D-2240
Tensile Strength, Yield 40.7 MPa
5900 psi
ASTM D-638
Tensile Modulus 3.34 GPa
484 ksi
ASTM D-638
Flexural Strength 73.1 MPa
10600 psi
ASTM D-790
Flexural Modulus 3.02 GPa
438 ksi
ASTM D-790
Izod Impact, Notched 8.92 J/cm

@Thickness 3.17 mm
16.7 ft-lb/in

@Thickness 0.125 in
ASTM D-256
Tensile Impact Strength 151 kJ/m²
72.0 ft-lb/in²
ASTM D-1822
Thermal Properties Metric English Comments
CTE, linear 64.8 µm/m-°C

@Temperature 20.0 °C
36.0 µin/in-°F

@Temperature 68.0 °F
ASTM D-696
Deflection Temperature at 0.46 MPa (66 psi) 75.6 °C
168 °F
ASTM D-648
Deflection Temperature at 1.8 MPa (264 psi) 72.2 °C
162 °F
ASTM D-648