Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 0.300 - 16.0 g/10 min | 0.300 - 16.0 g/10 min | Average value: 6.67 g/10 min Grade Count:26 |
Overview of materials for Acetal Copolymer, 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% ar.. |
|||
Melt Flow | 0.300 - 45.0 g/10 min | 0.300 - 45.0 g/10 min | Average value: 15.9 g/10 min Grade Count:42 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded". Each property range of values reported is m.. |
|||
Melt Flow | 0.300 - 80.0 g/10 min | 0.300 - 80.0 g/10 min | Average value: 17.1 g/10 min Grade Count:130 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant". Each property range of values rep.. |
|||
Melt Flow | 0.300 - 1500 g/10 min | 0.300 - 1500 g/10 min | Average value: 63.5 g/10 min Grade Count:103 |
Overview of materials for Polypropylene, Fiber Grade This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Fiber Grade". Each property range of values reported is minimum and maximum values of app.. |
|||
Melt Flow | 0.300 - 42.0 g/10 min | 0.300 - 42.0 g/10 min | Average value: 15.1 g/10 min Grade Count:15 |
Overview of materials for High Density Polyethylene (HDPE), Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Impact Grade". Each property range of values reported is minimum and m.. |
|||
Melt Flow | 0.300 g/10 min @Load 10.0 kg, Temperature 190 °C |
0.300 g/10 min @Load 22.0 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex HFFR 2004 Polyolefin, Halogen Free Notes: RoHS Compliant Features: Flame Retardant; Halogen Free Uses: Communication Wire Jacketing; Electronic Cable Jacketing; Security Cable JacketingAgency Ratings: IEC Unspecified Rating; ICEA Uns.. |
|||
Melt Flow | 0.300 g/10 min @Load 2.16 kg, Temperature 230 °C |
0.300 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex Telcar® OBC 2419B Thermoplastic Elastomer Notes: Telcar OBC has superior mechanical strength and higher elongation which will provide a tougher more durable finished product. Telcar OBC can be used in less demanding sealing applications. T.. |
|||
Melt Flow | 0.300 g/10 min @Load 2.16 kg, Temperature 230 °C |
0.300 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex Telcar® TL-1050-80 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Melt Flow | 0.300 g/10 min @Load 2.16 kg, Temperature 230 °C |
0.300 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex Telcar® TL-86-K986-A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Automotive Spec.. |
|||
Melt Flow | 0.300 - 7.00 g/10 min | 0.300 - 7.00 g/10 min | Average value: 2.70 g/10 min Grade Count:20 |
Overview of materials for Nylon, Flexible Alloy This property data is a summary of similar materials in the MatWeb database for the category "Nylon, Flexible Alloy". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Melt Flow | 0.300 - 58.0 g/10 min | 0.300 - 58.0 g/10 min | Average value: 13.3 g/10 min Grade Count:92 |
Overview of materials for Polyether Ester Elastomer This property data is a summary of similar materials in the MatWeb database for the category "Polyether Ester Elastomer". Each property range of values reported is minimum and maximum values of appr.. |
|||
Melt Flow | 0.300 - 140 g/10 min | 0.300 - 140 g/10 min | Average value: 12.4 g/10 min Grade Count:170 |
Overview of materials for Polypropylene, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Flame Retardant". Each property range of values reported is minimum and maximum values of.. |
|||
Melt Flow | 0.300 - 100 g/10 min | 0.300 - 100 g/10 min | Average value: 18.2 g/10 min Grade Count:222 |
Overview of materials for Polypropylene, Impact Modified; Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Impact Modified; Molded/Extruded". Each property range of values reported is minimum and .. |