Material Notes:
Notes: RoHS Compliant Features: Flame Retardant; Halogen Free Uses: Communication Wire Jacketing; Electronic Cable Jacketing; Security Cable JacketingAgency Ratings: IEC Unspecified Rating; ICEA Unspecified Rating Processing Method: Extrusion Forms: Pellets Additional Information: Ultimate Elongation Retained, UL 1581, Oven Aged, 7 days, 100°C: 80% Tensile Strength Retained, UL 1581, Oven Aged, 7 days, 100°C: 107% Cone Calorimeter at 50 kW/m2, Peak Heat Release Rate: 134 kW/m2 Cone Calorimeter at 50 kW/m2, Total Heat Released: 166 MJ/m2 Cone Calorimeter at 50 kW/m2, Peak Smoke: 0.6 1/m Cone Calorimeter at 50 kW/m2, Time to Sustained Ignition: 142 secInformation Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 1.52 g/cc
1.52 g/cc
ASTM D792
Melt Flow 0.300 g/10 min

@Load 10.0 kg,
Temperature 190 °C
0.300 g/10 min

@Load 22.0 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 65
65
10 seconds; ASTM D2240
Tensile Strength at Break 16.8 MPa
2430 psi
ASTM D638
Elongation at Break 100 %
100 %
ASTM D638
Thermal Properties Metric English Comments
Brittleness Temperature -25.0 °C
-13.0 °F
ASTM D746
Oxygen Index 48 %
48 %
ASTM D2863
Electrical Properties Metric English Comments
Volume Resistivity 6.60e+14 ohm-cm
6.60e+14 ohm-cm
ASTM D257
Dielectric Constant 3.72

@Frequency 1000 Hz
3.72

@Frequency 1000 Hz
ASTM D150
Dissipation Factor 0.0040

@Frequency 1000 Hz
0.0040

@Frequency 1000 Hz
ASTM D150
Descriptive Properties Value Comments
Appearance Opaque