Polymer Property : Melt Flow = 16.0 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 0.300 - 16.0 g/10 min
0.300 - 16.0 g/10 min
Average value: 6.67 g/10 min Grade Count:26
Overview of materials for Acetal Copolymer, 30% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% ar..
Melt Flow 1.00 - 16.0 g/10 min
1.00 - 16.0 g/10 min
Average value: 8.07 g/10 min Grade Count:7
Overview of materials for Polycarbonate/PET Polyester Blend, Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/PET Polyester Blend, Glass Reinforced". Each property range of values reported is minimum ..
Melt Flow 0.180 - 16.0 g/10 min
0.180 - 16.0 g/10 min
Average value: 5.81 g/10 min Grade Count:58
Overview of materials for Low Density Polyethylene (LDPE), Extrusion Grade
This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Extrusion Grade". Each property range of values reported is minimum and..
Melt Flow 1.00 - 16.0 g/10 min
1.00 - 16.0 g/10 min
Average value: 8.42 g/10 min Grade Count:6
Overview of materials for Polyphenylene Ether, 30% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 30% Glass Filled". Specific grades with glass content between 25% and 34% are inclu..
Melt Flow 0.700 - 16.0 g/10 min
0.700 - 16.0 g/10 min
Average value: 4.18 g/10 min Grade Count:124
Overview of materials for Acrylic, Impact Modified, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Impact Modified, Molded". Each property range of values reported is minimum and maximum values ..
Melt Flow 0.900 - 16.0 g/10 min
0.900 - 16.0 g/10 min
Average value: 7.14 g/10 min Grade Count:17
Overview of materials for Polypropylene, Glass Reinforced, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Glass Reinforced, Impact Modified". Each property range of values reported is minimum and..