Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 1.20 - 100 g/10 min | 1.20 - 100 g/10 min | Average value: 9.36 g/10 min Grade Count:116 |
Overview of materials for Polystyrene, Molded, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene". Each property range of values reported is minimum and maximum values of appropriate MatWeb.. |
|||
Melt Flow | 60 - 100 g/10 min @Load 2.16 kg, Temperature 170 °C |
60 - 100 g/10 min @Load 4.76 lb, Temperature 338 °F |
ISO 1133 |
Lubrizol Advanced Materials PEARLBOND® 523 Linear Thermoplastic Polyurethane Pearlbond™ 523 is a linear, polycaprolactone-copolyester polyurethane, supplied in form of white spherical granules with a very high crystallization rate and a very high thermoplasticity level... |
|||
Melt Flow | 60 - 100 g/10 min @Load 2.16 kg, Temperature 170 °C |
60 - 100 g/10 min @Load 4.76 lb, Temperature 338 °F |
ISO 1133 |
Lubrizol Advanced Materials PEARLBOND® 123 Linear Thermoplastic Polyurethane Pearlbond™ 123 is a linear, polycaprolactone-based polyurethane, supplied in form of small white granules, which combines an extremely high crystallization rate with a very high thermoplasticit.. |
|||
Melt Flow | 60 - 100 g/10 min @Load 2.16 kg, Temperature 170 °C |
60 - 100 g/10 min @Load 4.76 lb, Temperature 338 °F |
ISO 1133 |
Lubrizol Advanced Materials PEARLBOND® 503 Linear Thermoplastic Polyurethane Pearlbond™ 503 is a linear, polycaprolactone-copolyester polyurethane, supplied in form of white spherical granules with a high crystallization rate and a very high thermoplasticity level.Appli.. |
|||
Melt Flow | 1.00 - 100 g/10 min | 1.00 - 100 g/10 min | Average value: 12.2 g/10 min Grade Count:19 |
Overview of materials for Nylon 6, Heat Stabilized This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Heat Stabilized". Each property range of values reported is minimum and maximum values of appro.. |
|||
Melt Flow | 60 - 100 g/10 min @Load 2.16 kg, Temperature 170 °C |
60 - 100 g/10 min @Load 4.76 lb, Temperature 338 °F |
DDIN 53.735 |
Lubrizol Advanced Materials Pearlbond® D183 Thermoplastic Polyurethane
(discontinued **) The Pearlbond® grades are aromatic crystalline TPUs used for the production of heat activated shoe counters and toe puffs, and orthopedic products. The Pearlbond® grades are supplied in pellet fo.. |
|||
Melt Flow | 60 - 100 g/10 min @Load 2.16 kg, Temperature 170 °C |
60 - 100 g/10 min @Load 4.76 lb, Temperature 338 °F |
ISO 1133 |
Lubrizol Advanced Materials PEARLBOND® 103 Linear Thermoplastic Polyurethane Pearlbond™ 103 is a linear, polycaprolactone-based polyurethane, supplied in form of small white granules, which combines a very high crystallization rate with a very high thermoplasticity level. I.. |
|||
Melt Flow | 15.0 - 100 g/10 min | 15.0 - 100 g/10 min | Average value: 61.0 g/10 min Grade Count:5 |
Overview of materials for Nylon 6, MoS2 Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, MoS2 Filled". Each property range of values reported is minimum and maximum values of appropria.. |
|||
Melt Flow | 1.00 - 100 g/10 min | 1.00 - 100 g/10 min | Average value: 26.4 g/10 min Grade Count:55 |
Overview of materials for Nylon 6, 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 20% Glass Fiber Filled".Specific grades with glass content between 15% and 24% are included. Ea.. |
|||
Melt Flow | 0.300 - 100 g/10 min | 0.300 - 100 g/10 min | Average value: 18.2 g/10 min Grade Count:222 |
Overview of materials for Polypropylene, Impact Modified; Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Impact Modified; Molded/Extruded". Each property range of values reported is minimum and .. |
|||
Melt Flow | 0.500 - 100 g/10 min | 0.500 - 100 g/10 min | Average value: 15.2 g/10 min Grade Count:223 |
Overview of materials for Polypropylene, Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Mineral Reinforced". Each property range of values reported is minimum and maximum values.. |