Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 1300 cP @Shear Rate 11200 1/s, Temperature 200 °C |
1300 cP @Shear Rate 11200 1/s, Temperature 392 °F |
ASTM D3835 |
PolyOne Versaflex™ CL2003X Thermoplastic Elastomer (TPE) Versaflex™ CL2003X is an ultra-soft TPE designed for use in injection molding applications where exceptional clarity and ultra-soft properties are desired. New Product. Commercial specifications ha.. |
|||
Viscosity | 1300 cP @Temperature 22.2 °C |
1300 cP @Temperature 72.0 °F |
|
Northstar Polymers PNA-216 Curing Agent Information provided by Northstar Polymers. |
|||
Viscosity | 1300 - 1600 cP @Temperature 71.1 °C |
1300 - 1600 cP @Temperature 160 °F |
|
Northstar Polymers SBA-030 Polyester Curing Agent Information provided by Northstar Polymers. |
|||
Viscosity | 1300 - 1700 cP | 1300 - 1700 cP | 15% solution in MEK |
Lubrizol Advanced Materials Pearlstick® 49-46/15 Polyester based TPU
(discontinued **) TPUs for Solvent-based adhesivesApplications: Shoe, AutomotiveInformation provided by Merquinsa |
|||
Viscosity | 1300 cP @Temperature 25.0 °C |
1300 cP @Temperature 77.0 °F |
at 20 rpm vibration |
Permabond MM115 Anaerobic Threadlocker Permabond® MM115 Threadlocker is an excellent general purpose threadlocker and sealant. It is used for locking metal bolts, nuts and screws that may require disassembly for service and maintenance... |
|||
Viscosity | 1300 cP @Temperature 25.0 °C |
1300 cP @Temperature 77.0 °F |
at 20 rpm vibration |
Permabond MM115P Pure Anaerobic Threadlocker Permabond® MM115 PURE Threadlocker is an excellent general purpose threadlocker and sealant. It is used for locking metal bolts, nuts and screws that may require disassembly for service and mainten.. |
|||
Viscosity | 1300 cP | 1300 cP | ASTM D2293 |
Fibre Glast Saf-T-Poxy 2410 / 2183 Epoxy
(discontinued **) Information provided by Fibre Glast Developments Corporation. |
|||
Viscosity | 1300 cP @Temperature 25.0 °C |
1300 cP @Temperature 77.0 °F |
|
Momentive Performance Materials RTV6428 Dark Gray General Purpose Potting/Encapsulating Compound Two-part addition cure. Two-part addition cure RTV silicones can be cured very quickly with the use of high heat. Addition cure products have no cure by-products and can be used to unlimited depth.. |
|||
Viscosity | 1300 - 1700 cP @Temperature 23.0 °C |
1300 - 1700 cP @Temperature 73.4 °F |
|
Master Bond MB295 Cyanoacrylate Adhesive System Master Bond Polymer System MB295 is an ethyl cyanoacrylate adhesive system, recommended for use for combinations of plastics, lubber, ceramic or glass. Provides better general resistance to effects .. |
|||
Viscosity | 1300 cP @Temperature 160 °C |
1300 cP @Temperature 320 °F |
Melt; ETM 22-31 |
ExxonMobil ESCOREZ™ 1304 Petroleum Hydrocarbon Resin Premium aliphatic hydrocarbon resin which is designed to tackify a variety of adhesive polymers including EVA, metallocene polyolefines, APP, APAO, natural rubber, synthetic polyisoprene, polyisobut.. |
|||
Viscosity | 1300 cP | 1300 cP | dynamic |
Dow Corning 2601 COATING Anti-Graffiti, Anti-Stain, Easy Clean Coating for Interior and Exterior use.Information provided by Dow Corning |
|||
Viscosity | 1300 cP | 1300 cP | |
Abatron AboCast 7703-21/AboCure 7703-25 (E) Epoxy Adhesive and Casting Compound AboCast 7703-21/AboCure 7703-21 is an all-purpose clear, low-viscosity, variable-ratio epoxy adhesive and casting compound for electric and structural applications. As an Adhesive: it bonds permane.. |
|||
Viscosity | 1300 - 1700 cP | 1300 - 1700 cP | 15% solution in MEK |
Lubrizol Advanced Materials Pearlstick® 46-73/15 Polyester based TPU
(discontinued **) TPUs for Solvent-based adhesivesApplications: Shoe, OthersInformation provided by Merquinsa |
|||
Viscosity | 1300 - 3500 cP | 1300 - 3500 cP | |
Huntsman Araldite GZ 488 V-32 US Bisphenol A Epoxy Solution Weight per Epoxide (EEW, g/eq) 3570 to 5500. Max color is 3.Comments/Applications: Very high molecular weight solid epoxy (8,000 - 10,000), 35% solids in PM acetate. Outstanding adhesion, excellen.. |
|||
Viscosity | 1300 - 1500 cP @Temperature 60.0 °C |
1300 - 1500 cP @Temperature 140 °F |
|
C.O.I.M. DIEXTER® G235 Polyol Polyester Description: The DIEXTER® line of products offers a vast selection of polyol polyesters with different molecular weights and functions. DIEXTER® is sold for the production of polyurethanes in virt.. |
|||
Viscosity | 1300 cP | 1300 cP | Mixed; TM R050-12 |
Resinlab® EP1046FG Black Electronic Grade Epoxy Encapsulant Resinlab™ EP1046FG Black is a two part unfilled very fast curing electronic grade epoxy encapsulant designed for small castings (less than 25 grams). It cures very quickly with low exotherm to a to.. |
|||
Viscosity | 1300 cP | 1300 cP | Mixed; TM R050-12 |
Resinlab® EP1046FG Clear Electronic Grade Epoxy Encapsulant Resinlab™ EP1046FG Clear is a two part unfilled very fast curing electronic grade epoxy encapsulant designed for small castings (less than 25 grams). It cures very quickly with low exotherm to a to.. |