Resinlab™ EP1046FG Clear is a two part unfilled very fast curing electronic grade epoxy encapsulant designed for small castings (less than 25 grams). It cures very quickly with low exotherm to a tough, semi-rigid polymer matrix. Its low viscosity allows for good wicking and penetration into components and circuitry and also gives good air release. It has very good resistance to water, acids and bases and most organic solvents. It was especially formulated to a 1A:1B volume mix ratio for use in side-by-side dispensing cartridges and meter/mix and dispense equipment. EP1046FG Clear will reach handle cure at room temperature within 1 to 2 hours. Cure time can be accelerated by the application of heat after product has gelled. Times and temperatures from 30 minutes at 65°C to 10 minutes at 100°C are typical for small castings (less than 25 grams).Information Provided by Resinlab L.L.C., an Ellsworth Adhesives Company.
Physical Properties Metric English Comments
Specific Gravity 0.970 g/cc
0.970 g/cc
Part B; TM R050-16
1.05 g/cc
1.05 g/cc
Mixed; TM R050-16
1.14 g/cc
1.14 g/cc
Part A; TM R050-16
Water Absorption 0.29 %

@Time 86400 sec
0.29 %

@Time 24.0 hour
TM R050-35
Viscosity 1200 cP
1200 cP
Part A, RVT, #2, 2.5 rpm; TM R050-12
1300 cP
1300 cP
Mixed; TM R050-12
1400 cP
1400 cP
Part B, RVT, #2, 2.5 rpm; TM R050-12
Mechanical Properties Metric English Comments
Hardness, Shore D 85
85
TM R050-17
Tensile Strength at Break 24.1 MPa
3500 psi
TM R050-36
Tensile Strength, Ultimate 27.6 MPa
4000 psi
TM R050-36
Tensile Strength, Yield 10.3 MPa
1500 psi
TM R050-36
Elongation at Break 4.0 - 8.0 %
4.0 - 8.0 %
TM R050-36
Tensile Modulus 1.72 GPa
250 ksi
TM R050-36
Compressive Yield Strength 48.3 MPa
7000 psi
TM R050-38
Compressive Strength 96.5 MPa
14000 psi
Ultimate; TM R050-38
96.5 MPa
14000 psi
Break; TM R050-38
Compressive Modulus 1.38 GPa
200 ksi
TM R050-38
Adhesive Bond Strength 4.14 MPa
600 psi
Lap shear; 2024 T3 Al Abraded / MEK Wipe; TM R050-37
Thermal Properties Metric English Comments
CTE, linear 50.0 µm/m-°C
27.8 µin/in-°F
Thermal Conductivity 0.170 W/m-K
1.18 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 150 °C
302 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Glass Transition Temp, Tg 60.0 °C
140 °F
TM R050-25
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
clear; thickness not quantified
Electrical Properties Metric English Comments
Volume Resistivity 8.00e+14 ohm-cm
8.00e+14 ohm-cm
Dielectric Constant 4.5

@Frequency 100 Hz,
Temperature 25.0 °C
4.5

@Frequency 100 Hz,
Temperature 77.0 °F
Dielectric Strength 17.3 kV/mm
440 kV/in
Processing Properties Metric English Comments
Pot Life 2.0 - 4.0 min
2.0 - 4.0 min
Mass: 50g; TM R050-19
Descriptive Properties Value Comments
Color Clear
Mix Ratio 1:1
Volume
100:85
Weight