Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 1000 - 1500 cP | 1000 - 1500 cP | |
ND Industries SuperGlue Ethyl 316 Medium-high viscosity for gap fillingMeets military spec Mil-A-46050C Type II Class III |
|||
Viscosity | 800 - 1500 cP @Temperature 23.9 °C |
800 - 1500 cP @Temperature 75.0 °F |
|
TSE Industries EcoWIND® 200 Polyurethane Resin Filament Winding
(discontinued **) TSE-EcoWIND® resins are “Environmentally-Preferred Products” or EPP’s. They are a pair of polyurethane resins free of Styrene, and are “ultra-low” emitting during application. TSE-EcoWIND® re.. |
|||
Viscosity | 900 - 1500 cP | 900 - 1500 cP | |
Huntsman Araldite ECN 1400 Water-Based Adhesive/Coating Base Resin is ECN 1299. Typical Solids Content 40%. Mean Particle Size 4µm. Weight per Epoxide (EEW, g/eq), solids basis, 220 to 250.Comments/Applications: Adhesives; Fiber-Sizing; Textiles; A.. |
|||
Viscosity | 900 - 1500 cP | 900 - 1500 cP | 20% Toluene Solution at 25°C; BAM 922 |
Kraton® G1660 H (SEBS) Linear Triblock Copolymer Description: Kraton G1660 H is a linear triblock copolymer based on styrene and ethylene/butylene with a polystyrene content of 31%. It is supplied from North America in the physical form identified.. |
|||
Viscosity | 1000 - 1500 cP @Temperature 20.0 °C |
1000 - 1500 cP @Temperature 68.0 °F |
|
Lucite International Colacryl ® TS1173 Reactive Acrylic Syrup Lucite® Colacryl® TS1173 is a reactive polymer solution containing dissolved polymers, plasticiser and a polymerisation activator.Information provided by Lucite International |
|||
Viscosity | 1000 - 1500 cP | 1000 - 1500 cP | |
Huntsman Tactix 556 Multifunctional Resin Weight per Epoxide (EEW, g/eq) 215 to 235.Comments/Applications: Dicyclopentadiene based epoxy. Very low moisture pickup. Suggested for adhesives and composites used at elevated temperatures in a .. |
|||
Viscosity | 900 - 1500 cP | 900 - 1500 cP | 25% Toluene Solution at 25°C; KM 06 |
Kraton® D1102 A (SBS) Liner Block Copolymer Description: Kraton D1102 A is a clear, linear block copolymer based on styrene and butadiene with bound styrene of 29.5% mass. It is supplied from Europe in the physical form(s) identified below in.. |
|||
Viscosity | 500 - 1500 cP | 500 - 1500 cP | ASTM D803 |
SK Chemicals SKYTHANE® U0417E Adhesive (Dry Lamination) Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Viscosity | 500 - 1500 cP | 500 - 1500 cP | ASTM D803 |
SK Chemicals SKYTHANE® US518 Adhesive (Dry Lamination) Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Viscosity | 500 - 1500 cP | 500 - 1500 cP | RP-0596 |
Solvay ALCOCARE® 6012 Surfactant Description: NSF Registered product accepted for use as a hand washing and sanitizing compound (E-2 Rated Cleanser) for use in and around food processing areas. Sub-registration is required.Chemical.. |
|||
Viscosity | 1200 - 1500 cP | 1200 - 1500 cP | |
Master Bond Mastersil 151 Two Component Low Viscosity Silicone Compound Master Bond MasterSil 151 is a two component, low viscosity
silicone compound for high performance potting and
encapsulation. MasterSil 151 is an addition cured system and does not require exposure.. |
|||
Viscosity | 1200 - 1500 cP @Temperature 23.0 °C |
1200 - 1500 cP @Temperature 73.4 °F |
|
Master Bond UV10MED Biocompatible One Component UV Curable Adhesive System Master Bond UV10Med is a one part UV type system for bonding, sealing and coating. It fully passes USP Class VI testing requirements and features good optical clarity and physical properties as well.. |
|||
Viscosity | 100 - 1500 cP | 100 - 1500 cP | Milled Cement; Zeon Test #1377 |
Zeon Chemicals Nipol® 1472X Nitrile Powder and Crumb Elastomer Nipol 1472X is a copolymer of butadiene and acrylonitrile of medium-high acrylonitrile contnet modified to contain carboxyl groups. It contains sufficient antioxidant for normal storage conditions. .. |
|||
Viscosity | 1200 - 1500 cP @Temperature 23.9 °C |
1200 - 1500 cP @Temperature 75.0 °F |
|
TSE Industries EzNATE® 200 Polyurethane Resin TSE-EcoWIND® resins are “Environmentally-Preferred Products” or EPP’s. They are a pair of polyurethane resins free of Styrene, and are “ultra-low” emitting during application. TSE-EcoWIND® re.. |
|||
Viscosity | 1000 - 1500 cP @Temperature 23.0 °C |
1000 - 1500 cP @Temperature 73.4 °F |
100 rpm |
Epoxy Technology EPO-TEK® OG133-8 UV Cure Optical Epoxy Material Description: A single component, UV curable, thixotropic flexible epoxy adhesive/encapsulant designed for semiconductor and opto-electronic packaging. Glob top over IC and wire bonds, and .. |
|||
Viscosity | 1100 - 1500 cP | 1100 - 1500 cP | |
Aremco Aremco-Seal™ 617 High Temperature Glass Coating Glass-filled adhesive/sealer for use with porous ceramics and refractories to 1500 ºF (816 ºC). |
|||
Viscosity | 500 - 1500 cP | 500 - 1500 cP | |
Beijing Ranger Chem SM-634X80 Solvent Based Epoxy Resin Information provided by Beijing Ranger Chemical Co. |
|||
Viscosity | 1100 - 1500 cP | 1100 - 1500 cP | |
Aremco Aremco-Seal™ 617 High Temperature Specialty Coatings Glass Glass coating for producing hermetic seals in porous ceramics and refractories to 1450 ºF. Used for sealing high vacuum components, resistance temperature devices, and other electrical sensors. |
|||
Viscosity | 1000 - 1500 cP | 1000 - 1500 cP | |
Aremco Ceramacoat™ 845-BLK High Temperature Ceramic-Inorganic Coating Single part, waterborne, silicon-filled, phosphate-bonded, Jet Black coating for glass and quartz to 2000 ºF (1093 ºC). Primarily used for marking ceramic parts and coating automotive headlamps, s.. |
|||
Viscosity | 100 - 1500 cP | 100 - 1500 cP | |
Beijing Ranger Chem SM-601REK70 Solvent Based Epoxy Resin Information provided by Beijing Ranger Chemical Co. |
|||
Viscosity | 1200 - 1500 cP @Temperature 23.9 °C |
1200 - 1500 cP @Temperature 75.0 °F |
|
TSE Industries EzNATE® 200 Polyurethane Resin TSE-EcoWIND® resins are “Environmentally-Preferred Products” or EPP’s. They are a pair of polyurethane resins free of Styrene, and are “ultra-low” emitting during application. TSE-EcoWIND® re.. |
|||
Viscosity | 800 - 1500 cP @Temperature 23.0 °C |
800 - 1500 cP @Temperature 73.4 °F |
|
Master Bond UV15-7SP4DC One Component, Dual Cured, Flexible UV System Master Bond Polymer System UV15-7SP4DC is a one component, optically clear, dual cured flexible UV and/or heat curable polymer system with extended service capability of -80°F to +250°F. It cures .. |
|||
Viscosity | 500 - 1500 cP @Temperature 20.0 °C |
500 - 1500 cP @Temperature 68.0 °F |
15% solution in MEK; MQSA 40 A |
Lubrizol Advanced Materials Disperbond® D31S Thermoplastic Polyurethane
(discontinued **) Disperbond® originates from a new Merquinsa proprietary technology that produces linear, aromatic thermoplastic polyurethanes in pellet form. These TPUs can be dissolved in acetone. In a further .. |
|||
Viscosity | 1300 - 1500 cP @Temperature 60.0 °C |
1300 - 1500 cP @Temperature 140 °F |
|
C.O.I.M. DIEXTER® G235 Polyol Polyester Description: The DIEXTER® line of products offers a vast selection of polyol polyesters with different molecular weights and functions. DIEXTER® is sold for the production of polyurethanes in virt.. |
|||
Viscosity | 900 - 1500 cP @Temperature 25.0 °C |
900 - 1500 cP @Temperature 77.0 °F |
Uncured |
Permabond 947 Cyanoacrylate, low odor PERMABOND 947 is a low odor, non-fogging non-frosting alkoxyethyl cyanoacrylate. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate ad.. |