Polymer Property : Viscosity = 1700 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 1400 - 1700 cP
1400 - 1700 cP
Liquid State
Palm Labs Adhesives Turbo Fuse Series 170 (1000 Viscosity) Rapid Bonding Adhesive
Palm Lab's Cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE SERIES 170 advanced formula is designed to polymerize instantly by absorbing surface moisture. The product's performanc..
Viscosity 1400 - 1700 cP
1400 - 1700 cP
Liquid State
Palm Labs Adhesives TURBO FUSE SERIES 170 LOW ODOR/LOW BLOOM (1500 Viscosity) Rapid Bonding Adhesive
Palm Lab's Cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE SERIES 170 advanced formula is designed to polymerize instantly by absorbing surface moisture. The product's performanc..
Viscosity 1300 - 1700 cP
1300 - 1700 cP
15% solution in MEK
Lubrizol Advanced Materials Pearlstick® 49-46/15 Polyester based TPU  (discontinued **)
TPUs for Solvent-based adhesivesApplications: Shoe, AutomotiveInformation provided by Merquinsa
Viscosity 800 - 1700 cP
800 - 1700 cP
Huntsman Araldite AER 4100 N80 Brominated Resin
Weight per Epoxide (EEW, g/eq) 330 to 370. Max color is 5.Comments/Applications: Brominated epoxy resin solution in MEK, designed for use in high density multilayer circuit boards exhibiting high g..
Viscosity 1100 - 1700 cP
1100 - 1700 cP
Huntsman Araldite EPN 1139 Epoxy Phenol Novolac
Weight per Epoxide (EEW, g/eq) 172 to 179. Max color is 3.Comments/Applications: Epoxy phenol novolac for use in tank linings, high performance coatings. Used in matrix applications including fila..
Viscosity 1100 - 1700 cP
1100 - 1700 cP
Huntsman Araldite EPN 1179 Epoxy Phenol Novolac
Weight per Epoxide (EEW, g/eq) 172 to 179. Max color is 3.Comments/Applications: Epoxy functionality of 2.2. Viscosity between PY 307-1 and EPN 1138 or EPN 1180. Epoxy phenol novolac for use in ta..
Viscosity 900 - 1700 cP
900 - 1700 cP
25% Toluene Solution at 25°C; KM 06
Kraton® D1161 J (SIS) Linear Triblock Copolymer
Description: Kraton D1161 J Polymer is a clear, linear block copolymer based on styrene and isoprene with bound styrene of 15% mass. It is supplied from Japan in the physical form(s) identified in t..
Viscosity 800 - 1700 cP
800 - 1700 cP
Solvay RHODOLINE® DF-665 Surfactant
Description: Highly efficient mineral oil based defoamers for flat to gloss paints, quick process foam know down and high in-can persistency.Identification: OIL BASE DEFOAMERAvailable in: North Amer..
Viscosity 1300 - 1700 cP

@Temperature 23.0 °C
1300 - 1700 cP

@Temperature 73.4 °F
Master Bond MB295 Cyanoacrylate Adhesive System
Master Bond Polymer System MB295 is an ethyl cyanoacrylate adhesive system, recommended for use for combinations of plastics, lubber, ceramic or glass. Provides better general resistance to effects ..
Viscosity 1200 - 1700 cP

@Temperature 23.0 °C
1200 - 1700 cP

@Temperature 73.4 °F
100 rpm
Epoxy Technology EPO-TEK® OG142-112 UV Cure Optical Epoxy
Material Description: Single component, medium viscosity, UV curable epoxy for adhesive sealing and encapsulating fiber optic and optoelectronic packaging application. Replacement version of EPO-TE..
Viscosity 1000 - 1700 cP
1000 - 1700 cP
3M Pronto™ CA-9 Instant Adhesive
One-part, room-temperature curing adhesive that is ready-to-use without metering or mixing. Bonded parts reach handling strength in 5-10 seconds on many applications.A slower setting version of CA-..
Viscosity 1000 - 1700 cP
1000 - 1700 cP
3M Scotch-Weld™ CA9 Instant Adhesive
3M™ Scotch-Weld™ Instant Adhesives are single component, high strength cyanoacrylate adhesives. Slower setting version of CA8 for wire tacking and coil terminating. Meets CID A-A-3097, Type II, C..
Viscosity 1300 - 1700 cP
1300 - 1700 cP
15% solution in MEK
Lubrizol Advanced Materials Pearlstick® 46-73/15 Polyester based TPU  (discontinued **)
TPUs for Solvent-based adhesivesApplications: Shoe, OthersInformation provided by Merquinsa
Viscosity 1700 - 1700 cP

@Temperature 175 - 175 °C
1700 - 1700 cP

@Temperature 347 - 347 °F
Average value: 6480 cP Grade Count:1
Overview of materials for Epoxy Molding Compound
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Molding Compound". Each property range of values reported is minimum and maximum values of appropr..
Viscosity 1700 - 1700 cP

@Diameter 0.500 - 0.500 mm
1700 - 1700 cP

@Diameter 0.0197 - 0.0197 in
Average value: 6480 cP Grade Count:1
Overview of materials for Epoxy Molding Compound
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Molding Compound". Each property range of values reported is minimum and maximum values of appropr..