Polymer Property : Viscosity = 1600 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 1000 - 1600 cP
1000 - 1600 cP
cPs; 1% solution
Oceanchem Group Xanthan Gum Oil Drilling Grade
Information Provided by Oceanchem Group
Viscosity 1300 - 1600 cP

@Temperature 71.1 °C
1300 - 1600 cP

@Temperature 160 °F
Northstar Polymers SBA-030 Polyester Curing Agent
Information provided by Northstar Polymers.
Viscosity 800 - 1600 cP
800 - 1600 cP
25% Toluene Solution at 25°C; BAM 922
Kraton® D1161 P (SIS) Linear Triblock Copolymer
Description: Kraton D1161 P is a clear, linear triblock copolymer based on styrene and isoprene, with a polystyrene content of 15%. It is supplied from North America in the physical form identified:..
Viscosity 800 - 1600 cP
800 - 1600 cP
25% Toluene Solution at 25°C; KM 06
Kraton® D1102 J (SBS) Liner Block Copolymer
Description: Kraton D1102 J is a clear linear block copolymer based on styrene and butadiene with bound styrene of 30% mass. It is supplied from Japan in the physical form(s) identified below in the..
Viscosity 800 - 1600 cP

@Temperature 23.0 °C
800 - 1600 cP

@Temperature 73.4 °F
100 rpm
Epoxy Technology EPO-TEK® 302-3M Optically Transparent Epoxy
Product Description: EPO-TEK® 302-3M is a two component epoxy used for optical, medical, fiber optic, and semiconductor applications. The epoxy is good for adhesive joining, sealing, potting, or as..
Viscosity 800 - 1600 cP

@Temperature 23.0 °C
800 - 1600 cP

@Temperature 73.4 °F
100 rpm
Epoxy Technology EPO-TEK® E4110 Electrically Conductive, Silver Epoxy
Product Description: EPO-TEK® E4110 is an electrically conductive, silver-filled epoxy paste. This two component system is designed for low temperature curing from ambient to 80°C, although other..
Viscosity 1000 - 1600 cP
1000 - 1600 cP
Epoxyset Epoxiohm EO-21M-5 Electrically Conductive Epoxy Adhesive
EO-21M-5 is an electrically conductive & thermally conductive, silver filled epoxy adhesive. This two component system is designed to be cured at room temperature or the cure can be accelerated by e..
Viscosity 800 - 1600 cP
800 - 1600 cP
Beijing Ranger Chem SM-815CA Liquid Epoxy Resin
Information provided by Beijing Ranger Chemical Co.
Viscosity 1200 - 1600 cP
1200 - 1600 cP
Aremco Aremco-Seal™ 529HV High Temperature Specialty Coatings Silicone
High viscosity version, transparent silicone sealer with exceptional electrical and moisture resistance to 600°F (316°C). Ideal for use in cartridge heaters.