Dow Corning 2601 COATING

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer Dow Corning
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning 2601 COATING.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Anti-Graffiti, Anti-Stain, Easy Clean Coating for Interior and Exterior use.Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 1.11 g/cc

@Temperature 25.0 °C
1.11 g/cc

@Temperature 77.0 °F
Volatiles 43 %
43 %
Viscosity 1300 cP
1300 cP
dynamic
Thermal Properties Metric English Comments
Flash Point 26.7 °C
80.1 °F
closed cup
Processing Properties Metric English Comments
Shelf Life 18.0 Month
18.0 Month
Descriptive Properties Value Comments
Appearance clear
Color yellow
Water Resistant yes