Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 1100 cP @Temperature 25.0 °C |
1100 cP @Temperature 77.0 °F |
|
Northstar Polymers MPN-055 Polyether Prepolymer Information provided by Northstar Polymers. |
|||
Viscosity | 1100 - 1700 cP | 1100 - 1700 cP | |
Huntsman Araldite EPN 1139 Epoxy Phenol Novolac Weight per Epoxide (EEW, g/eq) 172 to 179. Max color is 3.Comments/Applications: Epoxy phenol novolac for use in tank linings, high performance coatings. Used in matrix applications including fila.. |
|||
Viscosity | 1100 - 1700 cP | 1100 - 1700 cP | |
Huntsman Araldite EPN 1179 Epoxy Phenol Novolac Weight per Epoxide (EEW, g/eq) 172 to 179. Max color is 3.Comments/Applications: Epoxy functionality of 2.2. Viscosity between PY 307-1 and EPN 1138 or EPN 1180. Epoxy phenol novolac for use in ta.. |
|||
Viscosity | 1100 cP | 1100 cP | |
Lord Adhesives 7700 Fast Setting, High Viscosity, Impact Resistant. Ethyl Cyanoacrylate Adhesive Lord Cyanoacrylate AdhesivesLord® Cyanoacrylate Adhesives were developed for production situations requiring instant bonds and immediate handling strength, particularly when bonding rubber, metal.. |
|||
Viscosity | 1100 cP | 1100 cP | 25% Toluene Solution at 25°C; BAM 922 |
Kraton® D1102 K (SBS) Liner Block Copolymer Description: Kraton D1102 K is a clear, linear triblock copolymer based on styrene and butadiene, with a polystyrene content of 28%. It is supplied from North America in the physical form identified.. |
|||
Viscosity | 1100 cP | 1100 cP | 25% Toluene Solution at 25°C; KM 06 |
Kraton® D1170 B (SIBS) Linear Triblock Copolymer Description: Kraton D1165 P is a clear, linear triblock copolymer based on styrene and isoprene with a polystyrene content of 30%. It is supplied from North America in the physical form identified: .. |
|||
Viscosity | 1100 - 1900 cP | 1100 - 1900 cP | 20% Toluene Solution at 25°C; BAM 922 |
Kraton® G1650 M (SEBS) Linear Triblock Copolymer Description: Kraton G1650 M is a clear, linear triblock copolymer based on styrene and ethylene/butylene with a polystyrene content of 30%. It is supplied from North America in the physical form ide.. |
|||
Viscosity | 1100 - 2500 cP @Time 7200 sec |
1100 - 2500 cP @Time 2.00 hour |
V-170-0 |
Solvay JAGUAR® HP 120 Surfactant Description: Best suited for use with solvents, even 100% ethanol based formulations. Jaguar HP 120 is a natural thickener and film former for hand sanitizersChemical Name: HYDROXYPROPYL GUARC.T.F.A.. |
|||
Viscosity | 1100 - 1800 cP @Temperature 25.0 °C |
1100 - 1800 cP @Temperature 77.0 °F |
|
Struktol STRUKSILON 8101 Silicone Stabilizer for PU-Rigid Foam STRUKSILON 8101 is used as a silicone stabilizer for production of polyurethane rigid foam. It is especially recommended for the use in PU-1- or PU-2-component spray foam applications.Applications: .. |
|||
Viscosity | 1100 cP @Temperature 25.0 °C |
1100 cP @Temperature 77.0 °F |
Mixed |
Trelleborg Emerson & Cuming Stycast® E-151-8 One-Component Epoxy Flexible Encapsulant Emerson & Cuming E-151-8 Stycast® One-Component Epoxy Flexible EncapsulantExcellent thermal shock and impact resistance. Good chemical resistance, high temperature, unfilled, low viscosity. Cure Ty.. |
|||
Viscosity | 1100 - 3500 cP | 1100 - 3500 cP | Dynamic |
Dow Corning Emulsifier 10 Emulsifier Emulsifier designed to prepare water-in-oil and water-in-silicone emulsions for use in skincare and topical pharmaceutical delivery applications.Information provided by Dow Corning |
|||
Viscosity | 1100 cP | 1100 cP | dynamic |
Dow Corning SE 1886 KIT Two-part, clear, 1:1, addition cure, low viscosity, good working time.Information provided by Dow Corning |
|||
Viscosity | 1100 cP @Temperature 180 °C |
1100 cP @Temperature 356 °F |
ETM 22-31 |
ExxonMobil ESCOREZ™ 5320 Petroleum Hydrocarbon Resin The Escorez 5300 series resins are water white cycloaliphatic hydrocarbon resins. They are designed to tackify a variety of adhesive polymers including EVA, SIS and SEBS block copolymers, APP an d A.. |
|||
Viscosity | 1100 - 1500 cP | 1100 - 1500 cP | |
Aremco Aremco-Seal™ 617 High Temperature Glass Coating Glass-filled adhesive/sealer for use with porous ceramics and refractories to 1500 ºF (816 ºC). |
|||
Viscosity | 1100 cP | 1100 cP | |
Abatron AboCast 8503-5/AboCure 8503-5 Colorless Epoxy AboCast 8503-5/AboCure 8503-5 is a faster hardening, colorless epoxy casting compound used for small castings and decoupage. It is a good choice for small castings, especially for analytical purpose.. |
|||
Viscosity | 1100 - 1500 cP | 1100 - 1500 cP | |
Aremco Aremco-Seal™ 617 High Temperature Specialty Coatings Glass Glass coating for producing hermetic seals in porous ceramics and refractories to 1450 ºF. Used for sealing high vacuum components, resistance temperature devices, and other electrical sensors. |