Material Notes:
AboCast 8503-5/AboCure 8503-5 is a faster hardening, colorless epoxy casting compound used for small castings and decoupage. It is a good choice for small castings, especially for analytical purposes and for small embedments, due to its faster reactivity. Suggested Uses: Transparent Casting, Embedding, Encapsulation, Potting, and Bonding. Casting display or experimental models without the high shrinkage of acrylic or other resins. Precise reproduction of anatomical or scientific models. Embedding organic, geologic, or metallurgic specimens. Encapsulation of electric, radioactive, or delicate components. Preservation or repair of artistic and historical objects. High-performance transparent table tops.
Physical Properties Metric English Comments
Viscosity 1100 cP
1100 cP
Mechanical Properties Metric English Comments
Hardness, Shore D 81
81
Tensile Strength at Break 56.5 MPa
8200 psi
Elongation at Break 15 %
15 %
Flexural Strength 77.9 MPa
11300 psi
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 50.0 °C
122 °F
Deflection Temp at unknown load
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
transparent; thickness not quantified
Processing Properties Metric English Comments
Pot Life 30 min

@Temperature 25.0 °C
30 min

@Temperature 77.0 °F
500 g
Descriptive Properties Value Comments
Hardening Time (min) 60-480
Parts by Weight (pbw) 100
AboCast
80
AboCure
Users viewing this material also viewed the following: