Kraton® D1102 K (SBS) Liner Block Copolymer

Category Polymer , Thermoplastic , Styrene-Butadiene , Styrene/Butadiene/Styrene (SBS)
Manufacturer Kraton
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kraton® D1102 K (SBS) Liner Block Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Kraton D1102 K is a clear, linear triblock copolymer based on styrene and butadiene, with a polystyrene content of 28%. It is supplied from North America in the physical form identified: Kraton D1102 KT - supplied as a dusted porous pelletKraton D1102 KU - supplied as an undusted porous pelletRegion: Europe, South America, Asia Pacific, Japan, and North America Uses: Kraton D1102 K is used as a modifier of bitumen or thermoplastics and in compound formulations. It is also suitable as an ingredient in formulating compounds for footwear applications and may be used in formulating adhesives, sealants and coatings. Applications: Adhesives, Sealant and Coatings; Bitumen Modification; Compounding and Personal Hygiene; Footwear; Impact Modification; Medical; Packaging and Polymod; Personal Care; and Roads and RoofingInformation provided by Kraton®
Physical Properties Metric English Comments
Specific Gravity 0.940 g/cc
0.940 g/cc
ASTM D4025
Bulk Density 0.449 g/cc
0.0162 lb/in³
Volatiles <= 0.70 %
<= 0.70 %
KM 04
Viscosity 1100 cP
1100 cP
25% Toluene Solution at 25°C; BAM 922
Melt Flow 14 g/10 min

@Load 5.00 kg,
Temperature 200 °C
14 g/10 min

@Load 11.0 lb,
Temperature 392 °F
Ash 0.20 - 0.40 %
0.20 - 0.40 %
Talc; BAM 908
Mechanical Properties Metric English Comments
Hardness, Shore A 66

@Time 10.0 sec
66

@Time 0.00278 hour
Typical values on polymer compression molded at 300°F; ASTM D2240
Tensile Strength 31.7 MPa
4600 psi
measured on films cast from a solution in toluene; ASTM D412
Elongation at Break 880 %
880 %
Measured on films cast from a solution in toluene; ASTM D412
300% Modulus 0.00276 GPa
0.400 ksi
Measured on films cast from a solution in toluene; ISO 37
Chemical Properties Metric English Comments
Diblock Content 17 %
17 %
Descriptive Properties Value Comments
Content Non-staining phenolic antioxidant
0.15-0.25%, KM 08
Polystyrene
28-30%, KM 03
Total Extractables
<1.0%, KM 05
Styrene/Rubber Ratio 28/72
Users viewing this material also viewed the following: