Huntsman Araldite EPN 1179 Epoxy Phenol Novolac

Category Polymer , Thermoset , Epoxy , Epoxy Encapsulant, Unreinforced
Manufacturer Huntsman, former Ciba Specialty Chemicals
Trade Name Araldite
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Huntsman Araldite EPN 1179 Epoxy Phenol Novolac.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Weight per Epoxide (EEW, g/eq) 172 to 179. Max color is 3.Comments/Applications: Epoxy functionality of 2.2. Viscosity between PY 307-1 and EPN 1138 or EPN 1180. Epoxy phenol novolac for use in tank linings, high performance coatings. Used in matrix applications; filament winding, casting, and pultrusion.Data provided by Ciba Specialty Chemicals.Ciba Specialty Chemicals has been acquired by Huntsman.
Physical Properties Metric English Comments
Viscosity 1100 - 1700 cP
1100 - 1700 cP