Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 1400 - 1900 cP | 1400 - 1900 cP | 25% Toluene Solution at 25°C; KM 06 |
Kraton® D1153 A (SBS) Liner Block Copolymer Description: Kraton D1153 A is a clear, linear block copolymer based on styrene and butadiene with bound styrene of 29.5% mass. It is supplied from Europe in the physical form(s) identified below in.. |
|||
Viscosity | 1400 - 1900 cP | 1400 - 1900 cP | 25% Toluene Solution at 25°C; KM 06 |
Kraton® D1153 E (SBS) Liner Block Copolymer Description: Kraton D1153 E is a clear, linear block copolymer based on styrene and butadiene with bound styrene of 29.5% mass. It is supplied from Europe in the physical form(s) identified below in.. |
|||
Viscosity | 1000 - 1900 cP | 1000 - 1900 cP | 20% Toluene Solution at 25°C; KM 06 |
Kraton® G1650 E (SEBS) Linear Triblock Copolymer Description: Kraton G1650 E is a clear linear triblock copolymer based on styrene and ethylene/butylene, S-E/B-S, with bound styrene of 29.2% mass. It is supplied from Europe in the physical forms i.. |
|||
Viscosity | 1100 - 1900 cP | 1100 - 1900 cP | 20% Toluene Solution at 25°C; BAM 922 |
Kraton® G1650 M (SEBS) Linear Triblock Copolymer Description: Kraton G1650 M is a clear, linear triblock copolymer based on styrene and ethylene/butylene with a polystyrene content of 30%. It is supplied from North America in the physical form ide.. |
|||
Viscosity | 1700 - 1900 cP @Temperature 40.0 °C |
1700 - 1900 cP @Temperature 104 °F |
|
Solvay ALKAMULS® S 20 Surfactant Identification: SORBITAN MONOLAURATECAS: 1338 – 39 – 2EINECS : 215 – 663 – 3Solubility: Dispersible in water. Soluble in most polar and aromatic solvents.Available in: Asia Pacif.. |
|||
Viscosity | 1400 - 1900 cP @Temperature 35.0 °C |
1400 - 1900 cP @Temperature 95.0 °F |
Dynamic viscosity |
C.O.I.M. PLAXTER® P 52 Polymeric Plasticizer Description: Formulated with PVC, it is used for the production of insulated cables and stretching films.Information provided by P.A.T. Products, Inc. |
|||
Viscosity | 1700 - 1900 cP @Shear Rate 230 1/s, Temperature 25.0 °C |
1700 - 1900 cP @Shear Rate 230 1/s, Temperature 77.0 °F |
Haake VT 550 PK1.1° |
Gwent Electronic Materials R2040227D1 Hot Melt Conductive Adhesive for Diagnostic Sensors This is a one-component water based polyurethane dispersion used for bonding unsupported PVC foils. This can be used in many different diagnostic applications such as test cards, assays and support.. |