Material Notes:
Description: Kraton G1650 M is a clear, linear triblock copolymer based on styrene and ethylene/butylene with a polystyrene content of 30%. It is supplied from North America in the physical form identified: Kraton G1650 MU - supplied as a powder.Region: Asia Pacific, Europe, Japan, North America, and South AmericaUses: Kraton G1650 M is used in compound formulations and as a modifier of thermoplastics. It may also find use in formulating adhesives, sealants, coatings and modified bitumens.Applications: Adhesives, Sealant and Coatings; Compounding and Personal Hygiene; Impact Modification; Medical; Packaging and Polymod; and Personal CareInformation provided by Kraton®
Physical Properties Metric English Comments
Specific Gravity 0.910 g/cc
0.910 g/cc
ASTM D2240
Bulk Density 0.224 g/cc
0.00809 lb/in³
Volatiles <= 1.0 %
<= 1.0 %
KM 04
Viscosity 1100 - 1900 cP
1100 - 1900 cP
20% Toluene Solution at 25°C; BAM 922
Melt Flow <= 1.0 g/10 min

@Load 5.00 kg,
Temperature 230 °C
<= 1.0 g/10 min

@Load 11.0 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 72

@Time 10.0 sec
72

@Time 0.00278 hour
ASTM D2240
Tensile Strength 34.5 MPa
5000 psi
ASTM D412
Elongation at Break 500 %
500 %
ASTM D412
300% Modulus 0.00552 GPa
0.801 ksi
ASTM D412
Descriptive Properties Value Comments
Content Non-staining phenolic antioxidant
0.03-0.1%, KM 08
Polystyrene
28.8-31.6%, Measured on the polymer before hydrogenation, KM 03
Total Extractables
<1.0%, KM 05
Styrene/Rubber Ratio 30/70