Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.00250 - 0.0170 cm/cm | 0.00250 - 0.0170 in/in | Average value: 0.00629 cm/cm Grade Count:25 |
Overview of materials for Polyetheretherketone, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Carbon Fiber Filled". Each property range of values reported is minimum and maximu.. |
|||
Linear Mold Shrinkage, Transverse | 0.00630 - 0.0170 cm/cm | 0.00630 - 0.0170 in/in | Average value: 0.0114 cm/cm Grade Count:21 |
Overview of materials for Nylon 66, Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Bead Filled". Each property range of values reported is minimum and maximum values of ap.. |
|||
Linear Mold Shrinkage, Transverse | 0.00700 - 0.0170 cm/cm | 0.00700 - 0.0170 in/in | Average value: 0.0106 cm/cm Grade Count:22 |
Overview of materials for Nylon 612, Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Glass Fiber Filler". Each property range of values reported is minimum and maximum values of .. |
|||
Linear Mold Shrinkage, Transverse | 0.00900 - 0.0170 cm/cm | 0.00900 - 0.0170 in/in | Average value: 0.0117 cm/cm Grade Count:4 |
Overview of materials for Nylon 46, Flame Retarded + Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Flame Retarded + Glass Fiber Reinforced". Each property range of values reported is minimum an.. |
|||
Linear Mold Shrinkage, Transverse | 0.000900 - 0.0170 cm/cm | 0.000900 - 0.0170 in/in | Average value: 0.00846 cm/cm Grade Count:200 |
Overview of materials for Nylon 6, 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. E.. |
|||
Linear Mold Shrinkage, Transverse | 0.000800 - 0.0170 cm/cm | 0.000800 - 0.0170 in/in | Average value: 0.00534 cm/cm Grade Count:241 |
Overview of materials for Polyetherimide (PEI) This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide". Each property range of values reported is minimum and maximum values of appropriate Mat.. |
|||
Linear Mold Shrinkage, Transverse | 0.00460 - 0.0170 cm/cm | 0.00460 - 0.0170 in/in | Average value: 0.0117 cm/cm Grade Count:29 |
Overview of materials for Polypropylene, Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Mineral Reinforced". Each property range of values reported is minimum and maximum values.. |
|||
Linear Mold Shrinkage, Transverse | 0.00500 - 0.0170 cm/cm | 0.00500 - 0.0170 in/in | Average value: 0.0113 cm/cm Grade Count:11 |
Overview of materials for Polytrimethylene Terephthalate (PTT) This property data is a summary of similar materials in the MatWeb database for the category "Polytrimethylene Terephthalate (PTT)". Each property range of values reported is minimum and maximum val.. |