Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.00200 - 0.00700 cm/cm | 0.00200 - 0.00700 in/in | Average value: 0.00429 cm/cm Grade Count:7 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled". Specific grades with glass content betwe.. |
|||
Linear Mold Shrinkage, Transverse | 0.00500 - 0.00700 cm/cm | 0.00500 - 0.00700 in/in | Average value: 0.00600 cm/cm Grade Count:8 |
Overview of materials for Polycarbonate/ASA Alloy, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ASA Alloy, Unreinforced". Each property range of values reported is minimum and maximum va.. |
|||
Linear Mold Shrinkage, Transverse | 0.00600 - 0.00700 cm/cm @Temperature 80.0 - 80.0 °C |
0.00600 - 0.00700 in/in @Temperature 176 - 176 °F |
Average value: 0.00650 cm/cm Grade Count:2 |
Overview of materials for Nylon 6, 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. E.. |
|||
Linear Mold Shrinkage, Transverse | 0.00400 - 0.00700 cm/cm | 0.00400 - 0.00700 in/in | Average value: 0.00529 cm/cm Grade Count:7 |
Overview of materials for Polycarbonate, Glass + PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Glass + PTFE Filled". Each property range of values reported is minimum and maximum value.. |