Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Linear Mold Shrinkage, Transverse = 0.0100 in/in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.00100 - 0.0100 cm/cm
0.00100 - 0.0100 in/in
Average value: 0.00566 cm/cm Grade Count:33
Overview of materials for Polyphthalamide (PPA), 50% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 50% Glass Fiber Reinforced". Each property range of values reported is minimum and maxi..
Linear Mold Shrinkage, Transverse 0.00300 - 0.0100 cm/cm
0.00300 - 0.0100 in/in
Average value: 0.00804 cm/cm Grade Count:5
Overview of materials for Polyphthalamide (PPA), Carbon Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Carbon Fiber". Each property range of values reported is minimum and maximum values of ..
Linear Mold Shrinkage, Transverse 0.000900 - 0.0100 cm/cm
0.000900 - 0.0100 in/in
Average value: 0.00647 cm/cm Grade Count:3
Overview of materials for Polystyrene + Polyphenylene Ether, Glass + Mineral Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene + Polyphenylene Ether, Glass + Mineral Filler". Each property range of values reported is mi..
Linear Mold Shrinkage, Transverse 0.00550 - 0.0100 cm/cm
0.00550 - 0.0100 in/in
Average value: 0.00700 cm/cm Grade Count:5
Overview of materials for Polyphenylene Ether, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Molded". Each property range of values reported is minimum and maximum values of ap..
Linear Mold Shrinkage, Transverse 0.00300 - 0.0100 cm/cm
0.00300 - 0.0100 in/in
Average value: 0.00668 cm/cm Grade Count:19
Overview of materials for Polycarbonate, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Impact Modified". Each property range of values reported is minimum and maximum values of..
Linear Mold Shrinkage, Transverse 0.00500 - 0.0100 cm/cm
0.00500 - 0.0100 in/in
Average value: 0.00727 cm/cm Grade Count:22
Overview of materials for Polycarbonate, UV Stabilized
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, UV Stabilized". Each property range of values reported is minimum and maximum values of a..
Linear Mold Shrinkage, Transverse 0.00300 - 0.0100 cm/cm
0.00300 - 0.0100 in/in
Average value: 0.00600 cm/cm Grade Count:47
Overview of materials for Polycarbonate/PET Polyester Blend
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/PET Polyester Blend". Each property range of values reported is minimum and maximum values..
Linear Mold Shrinkage, Transverse 0.00200 - 0.0100 cm/cm
0.00200 - 0.0100 in/in
Average value: 0.00740 cm/cm Grade Count:20
Overview of materials for PBT + ASA Blend, Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "PBT + ASA Blend, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum ..
Linear Mold Shrinkage, Transverse 0.00400 - 0.0100 cm/cm
0.00400 - 0.0100 in/in
Average value: 0.00650 cm/cm Grade Count:4
Overview of materials for Polyphenylene Sulfide (PPS) with 20% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 20% Glass Fiber Filler". Specific grades with glass content between 15%..
Linear Mold Shrinkage, Transverse 0.00150 - 0.0100 cm/cm
0.00150 - 0.0100 in/in
Average value: 0.00438 cm/cm Grade Count:41
Overview of materials for Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled". Each property range of values reported is mini..
Linear Mold Shrinkage, Transverse 0.00750 - 0.0100 cm/cm
0.00750 - 0.0100 in/in
Average value: 0.00860 cm/cm Grade Count:4
Overview of materials for Nylon 6, 20% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 20% Mineral Filled". Specific grades with primary filler content between 15% and 24% are includ..
Linear Mold Shrinkage, Transverse 0.00190 - 0.0100 cm/cm
0.00190 - 0.0100 in/in
Average value: 0.00715 cm/cm Grade Count:10
Overview of materials for Nylon 66/6, 20% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are incl..
Linear Mold Shrinkage, Transverse 0.00100 - 0.0100 cm/cm
0.00100 - 0.0100 in/in
Average value: 0.00425 cm/cm Grade Count:19
Overview of materials for Nylon 12, 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. ..
Linear Mold Shrinkage, Transverse 0.00100 - 0.0100 cm/cm

@Temperature 150 - 150 °C
0.00100 - 0.0100 in/in

@Temperature 302 - 302 °F
Average value: 0.00500 cm/cm Grade Count:17
Overview of materials for Polyethylene Terephthalate (PET), Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Unreinforced". Each property range of values reported is minimum and m..
Linear Mold Shrinkage, Transverse 0.00100 - 0.0100 cm/cm

@Time 900 - 900 sec
0.00100 - 0.0100 in/in

@Time 0.250 - 0.250 hour
Average value: 0.00500 cm/cm Grade Count:17
Overview of materials for Polyethylene Terephthalate (PET), Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Unreinforced". Each property range of values reported is minimum and m..
Linear Mold Shrinkage, Transverse 0.00500 - 0.0100 cm/cm
0.00500 - 0.0100 in/in
Average value: 0.00768 cm/cm Grade Count:11
Overview of materials for Polyethylene Terephthalate (PET), 50% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 50% Glass Reinforced". Specific grades with glass content between 45% ..
Linear Mold Shrinkage, Transverse 0.00530 - 0.0100 cm/cm
0.00530 - 0.0100 in/in
Average value: 0.00804 cm/cm Grade Count:19
Overview of materials for Polyethylene Terephthalate (PET), Glass/Mineral Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Glass/Mineral Reinforced". Each property range of values reported is m..
Linear Mold Shrinkage, Transverse 0.00800 - 0.0100 cm/cm

@Temperature 80.0 - 80.0 °C
0.00800 - 0.0100 in/in

@Temperature 176 - 176 °F
Average value: 0.00867 cm/cm Grade Count:3
Overview of materials for Nylon 6, 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 20% Glass Fiber Filled".Specific grades with glass content between 15% and 24% are included. Ea..