Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.18 - 1.38 g/cc | 1.18 - 1.38 g/cc | |
Parker Chomerics CHO-SHIELD® 4925 Conductive Coating Conductive Coating. CHO-SHIELD 4925 silver and nickel-filled conductive acrylic coating is intended for EMI shielding commercial thermoplastic housings. Its unique solvent system has been formulated.. |
|||
Specific Gravity | 1.32 - 1.38 g/cc | 1.32 - 1.38 g/cc | ASTM D792 |
S&E Specialty Polymers GA-1042LF PVC Application: UL bulletinized PVC based compound, suitable for injection molding application.Information provided by S&E Specialty Polymers |
|||
Specific Gravity | 1.34 - 1.38 g/cc | 1.34 - 1.38 g/cc | ASTM D 792 |
Karina E800-18/258-CR-AS Gray PVC Compound UV resistant PVC compoundInformation provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.32 - 1.38 g/cc @Thickness 1.57 mm |
1.32 - 1.38 g/cc @Thickness 0.0620 in |
ASTM D792 |
Industrial Laminates/Norplex NP611 Paper Base Laminate Description: Hot punching general-purpose phenolic grade. Mechanical properties approach those of NP610 with improved electrical properties and moisture resistance.Thickness Tested: 0.062", 0 125" a.. |
|||
Specific Gravity | 1.36 - 1.38 g/cc | 1.36 - 1.38 g/cc | |
LG Chemical PA1302 PVC General Description: PA1302, vinyl chloride copolymer with vinyl acetate exhibits excellent properties. It is easy to process and gives effective flow. Main Applications: Adhesive for sheet & film, .. |
|||
Specific Gravity | 1.32 - 1.38 g/cc | 1.32 - 1.38 g/cc | NBR NM-IEC 60811-1-3 |
Karina 08/240-FC-LMP Beige Color Concentrate for PVC Heavy metal free color concentrate recommended for application in electrical wire and cable PVC compounds. Also suitable for pigmentation of flexible and rigid PVC compounds for general purposes. .. |
|||
Specific Gravity | 1.32 - 1.38 g/cc | 1.32 - 1.38 g/cc | ASTM D 792 |
Karina E 20/15-RG-GE Cream Color Concentrate for PVC Color concentrate recommended for application in rigid PVC compounds for general purposes. Important Considerations:Heavy metal freeFormulated with organic and inorganic pigments PVC resin based (ca.. |
|||
Specific Gravity | 1.32 - 1.38 g/cc | 1.32 - 1.38 g/cc | NBR NM-IEC 60811-1-3 |
Karina E 36/234-FC-LMP Brown Color Concentrate for PVC Color concentrate recommended for application in PVC compounds for electrical wires and cables. Also suitable for pigmentation of flexible and rigid PVC compounds for general purposes.Important con.. |
|||
Specific Gravity | 1.25 - 1.38 g/cc | 1.25 - 1.38 g/cc | ASTM D 792 |
Karina 601-48/1-BY-IS-BZ Black PVC Compound Heavy metal free, weather resistant PVC compound recommended for injection and extrusion of automotive profiles.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.30 - 1.38 g/cc | 1.30 - 1.38 g/cc | ASTM D792 |
Spartech Royalite DKE 400 PVC/Acrylic Fire Rated Sheet Description: Fire Rated SheetInformation provided by Spartech. |
|||
Specific Gravity | 1.30 - 1.38 g/cc | 1.30 - 1.38 g/cc | ASTM D792 |
Spartech Royalite R60 PVC/Acrylic Aircraft Grade Sheet Description: Aircraft Grade SheetInformation provided by Spartech. |
|||
Specific Gravity | 1.34 - 1.38 g/cc | 1.34 - 1.38 g/cc | ASTM D-792 |
Axiall 8510 Moldings & Extrusions Flexible PVC A general purpose, semi-rigid T-molding and extrusion compound recommended for applications where a low gloss, matte finish is desired. The compound exhibits excellent abrasion resistance.Informati.. |
|||
Specific Gravity | 1.32 - 1.38 g/cc | 1.32 - 1.38 g/cc | ASTM D-792 |
Axiall MP-6585 Rigid PVC, Molding Georgia Gulf MP-6585 is an electrical grade rigid vinyl injection molding compound processing good strength, stiffness, toughness, and flow. In addition, it has excellent processing stability and s.. |
|||
Specific Gravity | 1.34 - 1.38 g/cc | 1.34 - 1.38 g/cc | ASTM D-792 |
Axiall 13870 Wire & Cable Flexible PVC Non-lead stabilized, 720 hour sunlight resistant insulation compound recommended for TW and 75C Class 43 applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 20.. |
|||
Specific Gravity | 1.34 - 1.38 g/cc | 1.34 - 1.38 g/cc | ASTM D-792 |
Axiall 13871 Wire & Cable Flexible PVC Non-lead stabilized, 720 hour sunlight resistant insulation compound recommended for TW and 75C Class 43 applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 20.. |
|||
Specific Gravity | 1.34 - 1.38 g/cc | 1.34 - 1.38 g/cc | ASTM D-792 |
Axiall 13872 Wire & Cable Flexible PVC Non-lead stabilized, 720 hour sunlight resistant insulation compound recommended for TW and 75°C Class 43 applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in .. |
|||
Specific Gravity | 1.34 - 1.38 g/cc | 1.34 - 1.38 g/cc | ASTM D-792 |
Axiall 14840 Wire & Cable Flexible PVC General purpose jacketing compound recommended for a maximum service temperature of 80°C.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.34 - 1.38 g/cc | 1.34 - 1.38 g/cc | ASTM D-792 |
Axiall 22880 Coax & Telecom Flexible PVC Flame retardant riser jacket over PVC or FR HDPE primaries.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.34 - 1.38 g/cc | 1.34 - 1.38 g/cc | ASTM D-792 |
Axiall 34551 Wire & Cable Flexible PVC TW, THW insulation also suitable for 105°C AWM, flex cords and Class 12/12B insulations.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.34 - 1.38 g/cc | 1.34 - 1.38 g/cc | ASTM D-792 |
Axiall 35061 Coax & Telecom Flexible PVC CMR jacket over PVC or flame retardant PE insulation with excellent low temperature properties.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.34 - 1.38 g/cc | 1.34 - 1.38 g/cc | ASTM D-792 |
Axiall 36631 Coax & Telecom Flexible PVC Semi-rigid, 80°C rated riser insulation compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.34 - 1.38 g/cc | 1.34 - 1.38 g/cc | ASTM D-792 |
Axiall 37740 Wire & Cable Flexible PVC 90°C rated compound designed for use as an inner and outer jacket in Teck 90 cables.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.34 - 1.38 g/cc | 1.34 - 1.38 g/cc | ASTM D-792 |
Axiall 8906 Moldings & Extrusions Flexible PVC General purpose extrusion compound recommended for applications requiring microbial resistance and good toughness.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.34 - 1.38 g/cc | 1.34 - 1.38 g/cc | ASTM D-792 |
Axiall 19750 Wire & Cable Flexible PVC 105°C rated insulation recommended for SPT cord applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.34 - 1.38 g/cc | 1.34 - 1.38 g/cc | ASTM D-792 |
Axiall 19840 Wire & Cable Flexible PVC 105°C rated insulation suitable for 1/64 wall. Recommended for AWM applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.34 - 1.38 g/cc | 1.34 - 1.38 g/cc | ASTM D-792 |
Axiall 22941 Coax & Telecom Flexible PVC Non-lead stabilized, 80C riser jacket.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.34 - 1.38 g/cc | 1.34 - 1.38 g/cc | ASTM D-792 |
Axiall 34311 Coax & Telecom Flexible PVC CMR riser jacket over PVC or flame retardant PE insulation. Recommended for 75C applications. UL recognized for 720 hour sunlight resistance in all colors.Information provided by Georgia GulfGeorg.. |
|||
Specific Gravity | 1.34 - 1.38 g/cc | 1.34 - 1.38 g/cc | ASTM D-792 |
Axiall 4425 Flexible PVC Non-lead stabilized high speed TWP automotive insulation. Rated for a maximum service temperature of 85°C. Suitable for SAE J1128, SAE 1560, Ford MIL 120A and Chrysler MS 7889; MS-DC16 Type A.Inf.. |
|||
Specific Gravity | 1.32 - 1.38 g/cc | 1.32 - 1.38 g/cc | ASTM D 792 |
Karina 06/706-RG-GE (CS) Blue Color Concentrate for PVC Heavy metal free color concentrate recommended for application in electrical wire and cable PVC compounds. Also suitable for pigmentation of flexible and rigid PVC compounds for general purposes. .. |
|||
Specific Gravity | 1.32 - 1.38 g/cc | 1.32 - 1.38 g/cc | ASTM D 792 |
Karina 802D18/441-CY-IS-AS-BZ Gray PVC Compound Heavy metal free PVC and weather resistant PVC compound, recommended for extrusion and injection of automotive profiles.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |