Axiall 34311 Coax & Telecom Flexible PVC

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Axiall
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall 34311 Coax & Telecom Flexible PVC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
CMR riser jacket over PVC or flame retardant PE insulation. Recommended for 75C applications. UL recognized for 720 hour sunlight resistance in all colors.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.34 - 1.38 g/cc
1.34 - 1.38 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore A 82 - 88
82 - 88
delayed; ASTM D-2240
89 - 95
89 - 95
ASTM D-2240
Tensile Strength, Yield 20.0 MPa
2900 psi
ASTM D-638
Elongation at Yield 262.4 %
262.4 %
Air Aging: 7 days @ 100°C; 75-mil plaques; UL 1581
320 %
320 %
ASTM D-638
100% Modulus 0.0117 GPa
1.70 ksi
ASTM D-638
Thermal Properties Metric English Comments
Brittleness Temperature -35.0 °C
-31.0 °F
ASTM D-746
Oxygen Index 31 %
31 %
ASTM D-638
Processing Properties Metric English Comments
Melt Temperature 185 °C
365 °F