Polymer Property : Specific Gravity = 1.36 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 1.36 g/cc
1.36 g/cc
ISO 1183
Radici Raditer® B RV 100 Polybutylene Terephthalate with 10% Glass fiber
Raditer® B RV 100 is a glass fiber reinforced thermoplastic polyester based on polybutylene terephthalate. The PBT compounds combine excellent thermal, mechanical, electrical and chemical properti..
Specific Gravity 1.36 g/cc
1.36 g/cc
ASTM D792
SABIC Innovative Plastics Lexan® LGN2000 PC (Asia Pacific)
Specific Gravity 1.36 g/cc
1.36 g/cc
ASTM D792
PolyOne Geon™ Vinyl Flexible R293AE Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Specific Gravity 1.36 g/cc
1.36 g/cc
ASTM D 792
RTP Company RTP 382 TFE 15 Polycarbonate (PC), Carbon Fiber - PTFE Lubricated
Specific Gravity 1.36 g/cc
1.36 g/cc
ASTM D 792
SABIC Innovative Plastics Lexan® SP7604 PC (Asia Pacific)
This data was supplied by SABIC-IP for the Asia Pacific region.
Specific Gravity 1.36 g/cc

@Temperature 23.0 °C
1.36 g/cc

@Temperature 73.4 °F
ASTM D792
Kingfa JE2-R2G20 Glass Fiber Reinforced ABS/PBT Alloy
Features:High stiffness, high hardnessGood mechanical strengthGood chemical resistanceGood size stabilityGood heat stabilityLow tendency to warpApplications:Optical appliance (camera, video)Sports a..
Specific Gravity 1.36 - 1.42 g/cc
1.36 - 1.42 g/cc
ASTM D 792
Karina 937-48/1-CY-IS-BZ Black PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Specific Gravity 1.36 g/cc
1.36 g/cc
ISO 1183
Gromax BFG30-DN00N1 Nylon 6 30% Glass Filled (Dry)
Information provided by Gromax Enterprises Corp.
Specific Gravity 1.36 g/cc
1.36 g/cc
ISO 1183
Lanxess Durethan® BKV 30 H2.0 EF 000000 Nylon 6, Glass Fiber Reinforced
PA 6, 30% glass fibers, injection molding, improved flowability, heat-aging stabilizedInformation provided by LANXESS.
Specific Gravity 1.36 g/cc
1.36 g/cc
Sylvin Technologies 9925-90 Natural PVC Molding Compound
Information provided by Sylvin Technologies Inc.
Specific Gravity 1.36 g/cc
1.36 g/cc
ASTM D 792
SABIC Innovative Plastics Ultem 1100FV PEI
Standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for th..
Specific Gravity 1.36 g/cc
1.36 g/cc
ASTM D 792
SABIC Innovative Plastics Ultem 1100R PEI
Standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Americas region.
Specific Gravity 1.36 g/cc
1.36 g/cc
ASTM D792
SABIC Innovative Plastics ULTEM HU1100 PEI (Asia Pacific)
Standard flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contac..
Specific Gravity 1.36 g/cc
1.36 g/cc
Shinil Chemical SHINSTRA PA-6 AG30N Structural Polymer Wheel Cover
SHINSTRA is the product line of structural polymer compound which exhibits excellent physical, mechanical, and thermal properties. Shinil uses the state-of-the-art dispersion and blending technolog..
Specific Gravity 1.36 g/cc
1.36 g/cc
ASTM D792
Teknor Apex APEX® 3310-80NT Polyvinyl Chloride, Flexible
Features: DEHP Plasticizer; Ethylene Oxide Sterilizable Uses: Food Service Applications; Medical/Healthcare Applications; Tubing Processing Forms: Extrusion Forms: PelletsInformation Provided by Tek..
Specific Gravity 1.36 g/cc
1.36 g/cc
ASTM D792
A. Schulman SCHULAMID® 66 MK30HI 30% Mineral Reinforced, Impact Modified Nylon 66
Information provided by A. Schulman.
Specific Gravity 1.36 g/cc
1.36 g/cc
ASTM D 792
RTP Company ESD 800 Acetal (POM), ESD Protection - Electrically Conductive
Specific Gravity 1.36 g/cc
1.36 g/cc
ASTM D792
A. Schulman POLYBATCH™ Tan LL60139/2 Concentrate Based In LLDPE
DescriptionPOLYBATCH® LL60139/2 is a tan color concentrate based in LLDPE. This concentrate was designed to provide opacity and color in blow molding applications. POLYBATCH® LL60139/2 is typic..
Specific Gravity 1.36 g/cc
1.36 g/cc
ASTM D792
A. Schulman POLYBATCH™ Tan LL60139/2 Concentrate Based In LLDPE
DescriptionPOLYBATCH® LL60139/2 is a tan color concentrate based in LLDPE. This concentrate was designed to provide opacity and color in blow molding applications. POLYBATCH® LL60139/2 is typic..
Specific Gravity 1.36 g/cc
1.36 g/cc
ASTM D 792
RTP Company RTP 205 HB Nylon 6/6 (PA), Glass Fiber - UL94 HB
Glass fiber reinforced nylon 6.6 offers significant improvements in strength, moduli and heat distortion temperature over the base resin. The HB series are UL94 HB certified materials.
Specific Gravity 1.36 - 1.40 g/cc
1.36 - 1.40 g/cc
ASTM D-792
Axiall 8820 Moldings & Extrusions Flexible PVC
General purpose extrusion and molding compound designed for use in weatherstrips, screen spline and flexible gaskets.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 201..
Specific Gravity 1.36 - 1.40 g/cc
1.36 - 1.40 g/cc
ASTM D-792
Axiall 11800 Wire & Cable Flexible PVC
Designed for 75°C rated cords and cord sets and other general purpose insulations.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Specific Gravity 1.36 - 1.40 g/cc
1.36 - 1.40 g/cc
ASTM D-792
Axiall 16930 Wire & Cable Flexible PVC
Non-lead stabilized tray cable jacketing compound. UL recognized component for 720 hour sunlight resistance in black only.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation ..
Specific Gravity 1.36 - 1.40 g/cc
1.36 - 1.40 g/cc
ASTM D-792
Axiall 8630 Moldings & Extrusions Flexible PVC
Extrusion compound recommended for extruded shapes and other applications where a matte finish is desired.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Specific Gravity 1.36 - 1.40 g/cc
1.36 - 1.40 g/cc
ASTM D-792
Axiall 10750 Wire & Cable Flexible PVC
General purpose 75C jacket compound with good low temperature properties.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Specific Gravity 1.36 - 1.40 g/cc
1.36 - 1.40 g/cc
ASTM D-792
Axiall 2192 Wire & Cable Flexible PVC
Non-lead stabilized SJTO, SJTOO oil resistant flexible cord jacket. UL recognized for 720 hour sunlight resistance in all colors.Information provided by Georgia GulfGeorgia Gulf became Axiall Corpo..
Specific Gravity 1.36 - 1.40 g/cc
1.36 - 1.40 g/cc
ASTM D-792
Axiall 8450 Moldings & Extrusions Flexible PVC
High durometer, general purpose extrusion compound formulated for microbial resistance.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Specific Gravity 1.36 g/cc
1.36 g/cc
ISO 1183
GEHR Plastics PVC-U Polyvinylchloride
Polyvinyl chloride is a flame retardant material with an exceptional chemical resistance and also with lower stress cracking. PVC-U shows high mechanical strength, tensile strength and the continuou..
Specific Gravity 1.36 g/cc
1.36 g/cc
ASTM D 792
RTP Company RTP 387 Polycarbonate (PC), Carbon Fiber