Axiall 8510 Moldings & Extrusions Flexible PVC

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Axiall
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall 8510 Moldings & Extrusions Flexible PVC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A general purpose, semi-rigid T-molding and extrusion compound recommended for applications where a low gloss, matte finish is desired. The compound exhibits excellent abrasion resistance.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.34 - 1.38 g/cc
1.34 - 1.38 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore D 48 - 54
48 - 54
delayed; ASTM D-2240
Tensile Strength, Yield 24.8 MPa
3600 psi
ASTM D-638
Elongation at Yield 285 %
285 %
ASTM D-638
100% Modulus 0.0186 GPa
2.70 ksi
ASTM D-638
Processing Properties Metric English Comments
Melt Temperature 191 °C
375 °F