Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Axiall 22941 Coax & Telecom Flexible PVC

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Axiall
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall 22941 Coax & Telecom Flexible PVC.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Non-lead stabilized, 80C riser jacket.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.34 - 1.38 g/cc
1.34 - 1.38 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore A 91 - 97
91 - 97
delayed; ASTM D-2240
Tensile Strength, Yield 20.7 MPa
3000 psi
ASTM D-638
Elongation at Yield 246.3 %
246.3 %
Air Aging: 168 hours @ 113°C; 30 mil slabs; UL 1581
300 %
300 %
ASTM D-638
100% Modulus 0.0155 GPa
2.25 ksi
ASTM D-638
Thermal Properties Metric English Comments
Brittleness Temperature -25.0 °C
-13.0 °F
ASTM D-746
Oxygen Index 32 %
32 %
ASTM D-638
Processing Properties Metric English Comments
Melt Temperature 191 °C
375 °F
Users viewing this material also viewed the following: