Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Axiall 13870 Wire & Cable Flexible PVC

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Wire and Cable Grade
Manufacturer Axiall
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall 13870 Wire & Cable Flexible PVC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Non-lead stabilized, 720 hour sunlight resistant insulation compound recommended for TW and 75C Class 43 applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.34 - 1.38 g/cc
1.34 - 1.38 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore A 84 - 90
84 - 90
delayed; ASTM D-2240
Tensile Strength, Yield 17.6 MPa
2550 psi
ASTM D-638
Elongation at Yield 272.7 %
272.7 %
Air Aging: 240 hours @ 100°C; 30 mil slabs; UL 1581
340 %
340 %
ASTM D-638
100% Modulus 0.0117 GPa
1.70 ksi
ASTM D-638
Thermal Properties Metric English Comments
Brittleness Temperature -28.0 °C
-18.4 °F
ASTM D-746
Oxygen Index 26 %
26 %
ASTM D-638
Electrical Properties Metric English Comments
Volume Resistivity 9.00e+14 ohm-cm
9.00e+14 ohm-cm
50% RH; ASTM D-257
Processing Properties Metric English Comments
Melt Temperature 182 °C
360 °F