Dow Corning Z-6094 SILANE

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer Dow Corning
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning Z-6094 SILANE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Aminoethylaminopropyltrimethoxysilane - H2NC2H4NHC3H6-Si(OCH3)3. High purity version of Z-6020, coupling agent.Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 1.02 g/cc

@Temperature 25.0 °C
1.02 g/cc

@Temperature 77.0 °F
Molecular Weight 222 g/mol
222 g/mol
Thermal Properties Metric English Comments
Boiling Point 264 °C
507 °F
Flash Point 43.0 °C
109 °F
closed cup
Descriptive Properties Value Comments
Active Content (%) 98
Adhesion to Plastic yes
Purity (%) 100