Physical Properties Metric English Comments
Specific Gravity 1.05 - 1.09 g/cc
1.05 - 1.09 g/cc
A component
Taiwan PU Corporation CPU-69-A/B Polyurethane Casting Elastomer
CPU-69-A consists of polyether polyols and other additives. CPU-69-b is an isocyanate prepolymer. Together they create compounds that cure under room temperature and have short working times, shor..
Specific Gravity 1.05 - 1.09 g/cc
1.05 - 1.09 g/cc
Asahi Glass Lumiflon LF-302 Solvent Soluble Fluoropolymer w/ Melamine hardening agent
Lumiflon was developed by Asahi Glass in 1982, and is unique being the first solvent soluble fluoropolymer. The FEVE based Lumiflon has a alternative copolymer. The complete inter-changeability betw..
Specific Gravity 1.02 - 1.09 g/cc
1.02 - 1.09 g/cc
ASTM D792
Buckeye Polymers BP RPP 2012 T BLK Polypropylene, Talc Filled
Product Information: Our Talc filled product lines exhibit excellent properties such as high stiffness, surface aesthetics, low coefficient of thermal expansion, low shrinkage, improved scratch and ..