Material Notes:
Features: Adhesion, GoodPaintableWeather Resistance, Good Forms:PelletsUses: Automotive ApplicationsSealsToothbrush HandlesInformation provided by Multibase
Physical Properties Metric English Comments
Specific Gravity 1.02 g/cc
1.02 g/cc
ASTM 792
Linear Mold Shrinkage 0.010 cm/cm
0.010 in/in
ASTM D955
Melt Flow 10 g/10 min

@Load 2.16 kg,
Temperature 230 °C
10 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 10.5 MPa
1530 psi
ASTM D638
Elongation at Break 600 %
600 %
ASTM D638
Flexural Modulus 0.0207 GPa
3.00 ksi
Secant; ASTM D790
Izod Impact, Notched NB
NB
ASTM D256
Tear Strength 36.8 kN/m
210 pli
ASTM D624
Thermal Properties Metric English Comments
Brittleness Temperature -60.0 °C
-76.0 °F
ASTM D746
Flame Spread <= 13 mm/min
<= 0.50 in/min
FM VSS-302
Users viewing this material also viewed the following: