Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PB1100-80 Polyurethane-based Biomedical Elastomer

Category Polymer , Thermoset , Polyurethane, TS , Rubber or Thermoset Elastomer (TSE)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PB1100-80 Polyurethane-based Biomedical Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.02 g/cc
1.02 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 80
80
ASTM D2240
Tensile Strength, Ultimate 31.7 MPa
4600 psi
ASTM D412
Tensile Strength, Yield 3.83 MPa
555 psi
at 100%; ASTM D412
Elongation at Break 590 %
590 %
ASTM D412
Tear Strength 57.8 kN/m
330 pli
die C; ASTM D624
Compression Set 25 - 30 %
25 - 30 %
ASTM D395