Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.016 - 0.022 cm/cm | 0.016 - 0.022 in/in | ASTM D955 |
PolyOne Versaflex™ HC MT555 Thermoplastic Elastomer (TPE) Versaflex™ HC MT555 is an easy processing material designed for applications where FDA compliance and medical testing is required. - Excellent Colorability - Soft TouchRear: 340 - 360F Center: 380 .. |
|||
Linear Mold Shrinkage, Flow | 0.016 - 0.020 cm/cm @Thickness 3.17 mm |
0.016 - 0.020 in/in @Thickness 0.125 in |
ASTM D955 |
Ravago Manufacturing Americas Hylon® N1000THLHF2 Nylon 6/6
(discontinued **) Available in North America Additive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Lubricated, Heat Stabilized, Impact Modifier and High FlowRoHS CompliantAuto Specifications: GM GMW16447P.. |
|||
Linear Mold Shrinkage, Flow | 0.016 cm/cm | 0.016 in/in | ISO 294-4 |
Akro-Plastic Akromid® S31 (3484) PA 6.10 Dry
(discontinued **) A characteristic property of AKROMID® S (PA 6.10) is that it has a renewable-resource content of up to 70 % and therefore fulfils the current definition of a bioplastic. The plant-based raw materia.. |
|||
Linear Mold Shrinkage, Flow | 0.016 cm/cm @Thickness 3.17 mm |
0.016 in/in @Thickness 0.125 in |
1/8" Section |
Lucent Polymers CPP-0107 Polypropylene Homopolymer Recycled ContentAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.016 cm/cm @Thickness 3.17 mm |
0.016 in/in @Thickness 0.125 in |
1/8" Section |
Lucent Polymers PPC-220 Polypropylene, Impact Modified Add "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.016 cm/cm @Thickness 3.17 mm |
0.016 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES Elastoblend® PA6 IM 835 HS L Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impact Modified and LubricatedProcessing Method: Injection MoldingInformat.. |
|||
Linear Mold Shrinkage, Flow | 0.016 cm/cm @Thickness 3.17 mm |
0.016 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES Elastoblend® PA6/6 HI BK Nylon 66 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubricant and Impact ModifiedUl File Number: E157318Appearance: BlackProce.. |
|||
Linear Mold Shrinkage, Flow | 0.016 cm/cm @Thickness 3.17 mm |
0.016 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES Elastoblend® PBT IM Availability: North AmericaForms: PelletsAdditive: Impact ModifierFeatures: Impact ModifiedProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.016 cm/cm @Thickness 3.17 mm |
0.016 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES HiFill® PA6 0137 S2 Availability: North AmericaForms: PelletsFiller/Reinforcement: MetalFeatures: High Specific GravityInformation provided by TP Composites, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.016 - 0.018 cm/cm @Thickness 3.20 mm |
0.016 - 0.018 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Xenoy® 6620 PBT+PC PBT+PC, Unreinforced, impact modified thermoplastic alloy. Outstanding impact at low temperature |
|||
Linear Mold Shrinkage, Flow | 0.016 cm/cm @Thickness 3.17 mm |
0.016 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES HiFill® PEEK 450 BK Availability: North AmericaForms: PelletsFeatures: High ViscosityAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.016 cm/cm @Thickness 3.17 mm |
0.016 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES Luriblend® POM CO X Acetal Availability: North AmericaForms: PelletsAdditive: LubricantFeatures: Lubricated, Good Wear Resistance and CopolymerInformation provided by TP Composites, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.016 cm/cm @Thickness 3.17 mm |
0.016 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES Elastoblend® PA6/6 IM X Nylon 66 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Lubricant and Impact ModifiedProcessing Method: Injection MoldingInformation provided by TP.. |
|||
Linear Mold Shrinkage, Flow | 0.016 cm/cm @Thickness 3.17 mm |
0.016 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES HiFill® PBT 0158 S Availability: North AmericaForms: PelletsFiller/Reinforcement: MetalInformation provided by TP Composites, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.016 cm/cm @Thickness 2.00 mm |
0.016 in/in @Thickness 0.0787 in |
TPE Method |
SCG Chemicals EL-Leneâ„¢ H5814J High Density Polyethylene Injection Molding Key Characteristics:Good processabilityHigh stiffnessHigh impact strengthBalanced properties between shrinkage and warpageOdorlessSafe for food contactRecommended Applications: General purpose inje.. |
|||
Linear Mold Shrinkage, Flow | 0.016 cm/cm | 0.016 in/in | ISO 294-4, 2577 |
EMS-Grivory Grivory® TSZ 3 PA666 Product description: Grilon TSZ 3 is a heat stabilized, normal viscosity, high impact modified PA66 + PA6 injection molding grade. Grilon TSZ 3 has the following important properties: Excellent toug.. |
|||
Linear Mold Shrinkage, Flow | 0.016 cm/cm | 0.016 in/in | ISO 294-4, 2577 |
EMS-Grivory Grivory® XE 4129 black 9020 PA610 Product description: Grilamid XE 4129 black 9020 is a high viscosity Polyamide 610 especially suitable for extrusion applications. A characteristic of tubes made out of this material is the high res.. |
|||
Linear Mold Shrinkage, Flow | 0.016 cm/cm | 0.016 in/in | ISO 294-4 2577 |
DuPont Performance Polymers Sorona® 3301V BK001 Polytrimethylene Terephthalate (PTT)
(Unverified Data**)& Unreinforced Renewably Sourced Polytrimethylene Terephthalate Sorona 3301V BK001 is an unreinforced black polytrimethylene terephthalate resin containing 35% renewably sourced ingredients by weight .. |
|||
Linear Mold Shrinkage, Flow | 0.016 cm/cm | 0.016 in/in | DAM; ISO 294-4 2577 |
DuPont Performance Polymers Zytel® FG53 NC010 Nylon 66
(Unverified Data**) Unreinforced High Viscosity Polyamide 66 with Developed for Food Contact Applications Information provided by DuPont Performance Polymers |
|||
Linear Mold Shrinkage, Flow | 0.016 - 0.020 cm/cm | 0.016 - 0.020 in/in | on Tensile Bar; E2P method |
Eurostar Staramide A40 PA66, Extrusion Staramide A40 is Unreinforced, High Viscosity Polyamide 66, Extrusion ResinInformation provided by Eurostar. |
|||
Linear Mold Shrinkage, Flow | 0.016 cm/cm @Thickness 4.00 mm |
0.016 in/in @Thickness 0.157 in |
E2P method |
Eurostar Starflam M10009AP PP, Flame Retardant, Injection Molding Starflam M10009AP is an Unfilled Flame Retardant high fluidity Polypropylene (Homo) Injection Molding ResinInformation provided by Eurostar. |
|||
Linear Mold Shrinkage, Flow | 0.016 - 0.018 cm/cm @Thickness 4.00 mm |
0.016 - 0.018 in/in @Thickness 0.157 in |
E2P method |
Eurostar Starflam PX07037 PA6, Flame Retardant, Injection Molded Starflam PX07037 is an Unfilled, Halogen Free and Red Phosphorous Free, Flame Retardant, Polyamide 6 Injection Molding Resin (IR laser marking grade)Information provided by Eurostar. |
|||
Linear Mold Shrinkage, Flow | 0.016 cm/cm | 0.016 in/in | Eurotec |
Eurotec® Tecodur® PB30 NL PBT, unfilled, natural, high viscosity, extrusion grade Information provided by Eurotec® |
|||
Linear Mold Shrinkage, Flow | 0.016 cm/cm | 0.016 in/in | Eurotec |
Eurotec® Tecodur® PB50 NL PBT, unfilled, natural, high viscosity Information provided by Eurotec® |
|||
Linear Mold Shrinkage, Flow | 0.016 cm/cm | 0.016 in/in | Eurotec |
Eurotec® Tecodur® PB70 NL PBT, unfilled, natural Information provided by Eurotec® |
|||
Linear Mold Shrinkage, Flow | 0.016 cm/cm | 0.016 in/in | ISO 294-4 2577 |
DuPont Performance Polymers Hytrel® HTR8223 BK320 Polyester Elastomer TPC-ET
(Unverified Data**) 42 Shore D High Viscosity Polyester Elastomer Developed for Blow MoldingInformation provided by DuPont Performance Polymers |
|||
Linear Mold Shrinkage, Flow | 0.016 cm/cm | 0.016 in/in | ISO 2577 |
BASF Ultramid® S3K Balance PA 610 (Conditioned) Description: BASF supplies polyamide 610 for processing by injection molding under the trade name Ultramid® Balance which is produced by polycondensation of hexamethylene diamine and sebacic acid. .. |
|||
Linear Mold Shrinkage, Flow | 0.016 cm/cm | 0.016 in/in | ISO 294-4 |
Azoty Tarnow™ Tarnamid® T-27 MCS Polyamide 6 - Colored Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.For colored parts produced by injection molding.Tarnamid® has the following .. |
|||
Linear Mold Shrinkage, Flow | 0.016 cm/cm | 0.016 in/in | ISO 294-4 |