Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.0035 - 0.0055 cm/cm @Thickness 3.20 mm |
0.0035 - 0.0055 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical LUPOY GP5056F PC/ABS+GF5%, Flame Retardance Description: Injection Molding, PC/ABS+GF5%, Flame Retardance, General PurposeApplication: IT/OA (Housing)CAS: 103598-77-2, 9003-56-9, 68928-70-1, 1309-64-4 and 65997-17-3Information provided by LG .. |
|||
Linear Mold Shrinkage, Flow | 0.0030 - 0.0055 cm/cm | 0.0030 - 0.0055 in/in | |
LATI Laramid G/35 PPA, 35% Glass Fiber Reinforced Semi-aromatic polyamide (PPA) based compound. Glass fibers. Very good thermal properties. Good chemical resistance. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; .. |
|||
Linear Mold Shrinkage, Flow | 0.0035 - 0.0055 cm/cm | 0.0035 - 0.0055 in/in | |
LATI Latamid 12 G/50 PA 12, 50% Glass Fiber Reinforced Polyamide 12 (PA12) based compound. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p.A. |
|||
Linear Mold Shrinkage, Flow | 0.0035 - 0.0055 cm/cm | 0.0035 - 0.0055 in/in | |
LATI Latamid 6 H2 G/30-V0HF1 PA 6, 30% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Very good electrical properties.Availability: Africa &.. |
|||
Linear Mold Shrinkage, Flow | 0.0025 - 0.0055 cm/cm | 0.0025 - 0.0055 in/in | |
LATI Latamid 66 H2 G/50-V0KB1 PA 66, 50% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with red phosphorous.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInf.. |
|||
Linear Mold Shrinkage, Flow | 0.0025 - 0.0055 cm/cm | 0.0025 - 0.0055 in/in | |
LATI Latamid 66 H2 G/60 PA 66, 60% Glass Fiber Reinforced, Heat Stabilized Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termopl.. |
|||
Linear Mold Shrinkage, Flow | 0.0030 - 0.0055 cm/cm | 0.0030 - 0.0055 in/in | |
LATI Kelon® B FR H CET/30-V0 PA 6, Mineral Reinforced, Flame Retardant, Heat Stabilized Polyamide 6 (PA6) based compound. Heat stabilized. Mineral filler. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Low thermal expansion coefficient. Very high dimensional stab.. |
|||
Linear Mold Shrinkage, Flow | 0.0035 - 0.0055 cm/cm | 0.0035 - 0.0055 in/in | |
LATI Kelon® B H CETG/300 PA 6, Glass/Mineral Reinforced, Heat Stabilized Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers / Mineral filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati I.. |
|||
Linear Mold Shrinkage, Flow | 0.0040 - 0.0055 cm/cm | 0.0040 - 0.0055 in/in | |
LATI Lapex A G/10 PES, 10% Glass Fiber Reinforced Polyether Sulfone (PES) based compound. Glass fibers. Low smoke density and low toxicity index. Very high dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin Americ.. |
|||
Linear Mold Shrinkage, Flow | 0.0040 - 0.0055 cm/cm | 0.0040 - 0.0055 in/in | |
LATI Lapex R G/20 PPSU, 20% Glass Reinforced Polyphenylene Sulfone (PPSU) based compound. Glass fibers. Low smoke density and low toxicity index. Very high dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin A.. |
|||
Linear Mold Shrinkage, Flow | 0.0030 - 0.0055 cm/cm | 0.0030 - 0.0055 in/in | |
LATI Latan 13 K/30 POM, 30% Carbon Fiber Reinforced Polyoxymethylene (POM) based compound. Carbon fiber. Medium viscosity. Good tribological properties.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation .. |
|||
Linear Mold Shrinkage, Flow | 0.0030 - 0.0055 cm/cm | 0.0030 - 0.0055 in/in | |
LATI Later 4 G/30 PBT, 30% Glass Fiber Reinforced Polybutylene Terephthalate (PBT) based compound. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplast.. |
|||
Linear Mold Shrinkage, Flow | 0.0025 - 0.0055 cm/cm | 0.0025 - 0.0055 in/in | |
LATI Laticonther 82 CP1/800 PA12 High thermal conductivity product based on Polyamide 12 (PA12). Special fillerAvailability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indus.. |
|||
Linear Mold Shrinkage, Flow | 0.0015 - 0.0055 cm/cm | 0.0015 - 0.0055 in/in | |
LATI Latigea B01 L/07 Bio-Polymer Bio-Polymer (PLA, PHB, ...) based compound. Wood flour. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p.. |
|||
Linear Mold Shrinkage, Flow | 0.0040 - 0.0055 cm/cm | 0.0040 - 0.0055 in/in | |
LATI Latilub 62-01M G/30 PA6, 30% Glass Fiber Reinforced Self-lubricating product based on Polyamide 6 (PA6). Molybdenum disulphide. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided b.. |
|||
Linear Mold Shrinkage, Flow | 0.0035 - 0.0055 cm/cm | 0.0035 - 0.0055 in/in | |
LATI Latilub 66-10T K/10 PA66, 10% Carbon Fiber Reinforced, PTFE Filled Self-lubricating product based on Polyamide 66 (PA66). PTFE. Carbon fiber.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria.. |
|||
Linear Mold Shrinkage, Flow | 0.0035 - 0.0055 cm/cm | 0.0035 - 0.0055 in/in | |
LATI Latimass 62-07 D025 PA6, Impact Modified Specific density compound based on Polyamide 6 (PA6), impact modified. Special filler.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by La.. |
|||
Linear Mold Shrinkage, Flow | 0.0030 - 0.0055 cm/cm | 0.0030 - 0.0055 in/in | |
LATI Latiohm 62-03 PD01 G/20 PPA, 20% Glass Fiber Reinforced Semiconductive/dissipative product based on Polyamide 6 (PA6). Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indust.. |
|||
Linear Mold Shrinkage, Flow | 0.0040 - 0.0055 cm/cm | 0.0040 - 0.0055 in/in | |
LATI Latiohm 62-08 PD02 G/30 PPA, 30% Glass Fiber Reinforced Dissipative product based on Polyamide 6 (PA6). Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplast.. |
|||
Linear Mold Shrinkage, Flow | 0.0040 - 0.0055 cm/cm | 0.0040 - 0.0055 in/in | |
LATI Latistat 62-06 K/10 PA6, 10% Carbon Fiber Reinforced Dissipative product based on Polyamide 6 (PA6). Carbon fiber. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplasti.. |
|||
Linear Mold Shrinkage, Flow | 0.0045 - 0.0055 cm/cm @Thickness 3.20 mm |
0.0045 - 0.0055 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL PX138H PPE+HIPS (Asia Pacific) Modified PPO Resin with 20% Glass Fibre Reinforced |
|||
Linear Mold Shrinkage, Flow | 0.0035 - 0.0055 cm/cm | 0.0035 - 0.0055 in/in | ISO DIS 294-4 |
Wellman Wellamid® GF1497-BK 43% Glass Fiber Reinforced, Silicone Lubricated Nylon 66 Description: Glass Fiber Reinforced, Silicone Lubricated Nylon 66Information provided by Wellman. |
|||
Linear Mold Shrinkage, Flow | 0.0025 - 0.0055 cm/cm | 0.0025 - 0.0055 in/in | ISO DIS 294-4 |
Wellman Wellamid® GF1758-BK2 33% Glass Fiber Reinforced Nylon 66 Description: Glass Fiber Reinforced Nylon 66Information provided by Wellman. |
|||
Linear Mold Shrinkage, Flow | 0.0025 - 0.0055 cm/cm | 0.0025 - 0.0055 in/in | ISO DIS 294-4 |
Wellman Wellamid® MRGF25/15 22H-NBK1 40% Mineral/Glass Reinforced Nylon 66 Description: Mineral/Glass Reinforced Nylon 66Information provided by Wellman. |
|||
Linear Mold Shrinkage, Flow | 0.0035 - 0.0055 cm/cm | 0.0035 - 0.0055 in/in | ISO DIS 294-4 |
Wellman Wellamid® WE1410 43% Glass Fiber Reinforced Nylon 66 Description: Glass Fiber Reinforced Nylon 66Information provided by Wellman. |
|||
Linear Mold Shrinkage, Flow | 0.0035 - 0.0055 cm/cm | 0.0035 - 0.0055 in/in | on Tensile Bar; E2P method |
Eurostar Starflam BFR430A PA6, Glass Fiber Filled, Flame Retardant, Injection Molded Starflam BFR430A is a Flame Retardant, Glass Fiber Reinforced Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Linear Mold Shrinkage, Flow | 0.0030 - 0.0055 cm/cm | 0.0030 - 0.0055 in/in | |
LATI Latilub 88/10-15T G/30 PEEK, 30% Glass Fiber Reinforced, PTFE Filled Self-lubricating product based on Polyetheretherketone (PEEK). PTFE. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati I.. |
|||
Linear Mold Shrinkage, Flow | 0.0035 - 0.0055 cm/cm | 0.0035 - 0.0055 in/in | |
LATI Latimass 62-01 D025 PA6 Specific density compound based on Polyamide 6 (PA6). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Ter.. |
|||
Linear Mold Shrinkage, Flow | 0.0030 - 0.0055 cm/cm | 0.0030 - 0.0055 in/in | |
LATI Latiohm 66-04 PD01 G/25-V0CT1 PA66, 25% Glass Fiber Reinforced, Flame Retardant Semiconductive/dissipative product based on Polyamide 66 (PA66). Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle East; Asia Pacific;.. |
|||
Linear Mold Shrinkage, Flow | 0.0035 - 0.0055 cm/cm | 0.0035 - 0.0055 in/in | |
LATI Latiohm 66-10 H2 CNT G/35 PA66, 35% Glass Fiber Reinforced, Heat Stabilized Semiconductive/dissipative product based on Polyamide 66 (PA66). Heat stabilized. Carbon nanotubes. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North Ameri.. |