Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LATI Laticonther 82 CP1/800 PA12

Category Polymer , Thermoplastic , Nylon , Nylon 12
Manufacturer LATI
Trade Name Laticonther
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LATI Laticonther 82 CP1/800 PA12.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High thermal conductivity product based on Polyamide 12 (PA12). Special fillerAvailability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p.A.
Physical Properties Metric English Comments
Density 2.14 g/cc
0.0773 lb/in³
Linear Mold Shrinkage, Flow 0.0025 - 0.0055 cm/cm
0.0025 - 0.0055 in/in
Linear Mold Shrinkage, Transverse 0.0025 - 0.0055 cm/cm
0.0025 - 0.0055 in/in
Mechanical Properties Metric English Comments
Tensile Strength at Break 45.0 MPa
6530 psi
Elongation at Break 0.60 %
0.60 %
Tensile Modulus 12.8 GPa
1860 ksi
Charpy Impact Unnotched 0.500 J/cm²
2.38 ft-lb/in²
Charpy Impact, Notched 0.150 J/cm²
0.714 ft-lb/in²
Thermal Properties Metric English Comments
Thermal Conductivity 9.50 W/m-K
65.9 BTU-in/hr-ft²-°F
Longitudinal
Deflection Temperature at 0.46 MPa (66 psi) 170 °C
338 °F
Deflection Temperature at 1.8 MPa (264 psi) 150 °C
302 °F
Vicat Softening Point 180 °C

@Load 5.00 kg
356 °F

@Load 11.0 lb
Processing Properties Metric English Comments
Melt Temperature 250 - 270 °C
482 - 518 °F
Mold Temperature 70.0 - 90.0 °C
158 - 194 °F
Drying Temperature 70.0 - 90.0 °C

@Time 10800 sec
158 - 194 °F

@Time 3.00 hour
Descriptive Properties Value Comments
ISO Shrinkage - Pressure 60 MPa
Copyright © lookpolymers.com All Rights Reserved