Ineos H38K-00 Polypropylene Homopolymer, Fiber Grade  (discontinued **)

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Fiber Grade
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ineos H38K-00 Polypropylene Homopolymer, Fiber Grade  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Suggested fabrication methods: Fiber spinningFeatures: Very high speed spinning, Low gas fade, Low smokeTypical applications: Spunbound fabricsComplies with FDA specification, Title 21, CFR 177.1520.Typical property data below from injection molded samples.The polypropylene and polyethylene products of BP Amoco have been moved to the Innovene Division in 2005.
Physical Properties Metric English Comments
Density 0.886 - 0.926 g/cc
0.0320 - 0.0335 lb/in³
ASTM D1505
Water Absorption <= 0.010 %
<= 0.010 %
24 hours; ASTM D570
Linear Mold Shrinkage 0.010 - 0.025 cm/cm
0.010 - 0.025 in/in
ASTM D955
Melt Flow 38 g/10 min

@Load 2.16 kg,
Temperature 230 °C
38 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 79 - 108
79 - 108
Normal range for injection molding resins; ASTM D785
Tensile Strength, Yield 33.0 MPa
4790 psi
ASTM D638
Elongation at Break 20 %
20 %
ASTM D638
Elongation at Yield 9.0 %
9.0 %
ASTM D638
Flexural Modulus 1.38 GPa
200 ksi
ASTM D790A
Izod Impact, Notched 0.200 - 0.300 J/cm

@Diameter 3.17 mm
0.375 - 0.562 ft-lb/in

@Diameter 0.125 in
bar; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 93.0 °C
199 °F
ASTM D648
Descriptive Properties Value Comments
Process Fiber Spinning