Material Notes:
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Good Flexibility, General Purpose, Ultra High MW, Recyclable, Good Thermal Stability, Good Weather ResistanceUses- Footwear, Tubing, Gaskets, Weatherstripping, hose, Wheels, SealsForms-PelletsProcessing-Extrusion, Injection MoldingInformation provided by Teknor Apex Company
Physical Properties Metric English Comments
Specific Gravity 1.07 g/cc
1.07 g/cc
23°C; ASTM D792
Linear Mold Shrinkage 0.010 - 0.025 cm/cm
0.010 - 0.025 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Shore A 35
35
15 seconds; ASTM D2240
Tensile Strength, Yield 2.07 MPa
300 psi
100%; ASTM D412
6.21 MPa
900 psi
ASTM D412
Elongation at Break 390 %
390 %
ASTM D412
Tear Strength 19.3 kN/m
110 pli
Die C; ASTM D624
Compression Set 23 %
23 %
73°F, 22 hr.; ASTM D395
61 %
61 %
158°F, 22 hr.; ASTM D395
Thermal Properties Metric English Comments
Brittleness Temperature -57.2 °C
-71.0 °F
ASTM D746
Processing Properties Metric English Comments
Rear Barrel Temperature 160 - 177 °C
320 - 350 °F
Middle Barrel Temperature 160 - 177 °C
320 - 350 °F
Front Barrel Temperature 160 - 177 °C
320 - 350 °F
Mold Temperature 23.9 - 51.7 °C
75.0 - 125 °F
Back Pressure 0.345 - 1.03 MPa
50.0 - 150 psi
Descriptive Properties Value Comments
Screw Compression Ratio 2:1-3:1
Screw L/D Ratio 20:1- 24:1
Suggested Max Regrind, % 20