Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.020 cm/cm | 0.020 in/in | ASTM D955 |
Network Polymers Kepital® F20-03 Description: Natural Acetal CopolymerInformation provided by Network Polymers Inc. |
|||
Linear Mold Shrinkage | 0.020 - 0.030 cm/cm @Thickness 3.17 mm |
0.020 - 0.030 in/in @Thickness 0.125 in |
ASTM D955 |
RTP Company RTP 800 TFE 10 SI 2 Acetal (POM), PTFE Lubricated - Silicone Lubricated |
|||
Linear Mold Shrinkage | 0.020 - 0.030 cm/cm @Thickness 3.17 mm |
0.020 - 0.030 in/in @Thickness 0.125 in |
ASTM D955 |
RTP Company RTP 800 TFE 10 SI 2 DEL Acetal (POM), PTFE Lubricated - Silicone Lubricated - Homopolymer |
|||
Linear Mold Shrinkage | 0.020 cm/cm @Thickness 3.17 mm |
0.020 in/in @Thickness 0.125 in |
ASTM D955 |
RTP Company RTP 800 TFE 15 DEL Acetal (POM), PTFE Lubricated |
|||
Linear Mold Shrinkage | 0.020 - 0.028 cm/cm @Thickness 3.17 mm |
0.020 - 0.028 in/in @Thickness 0.125 in |
ASTM D955 |
RTP Company RTP 841 Acetal (POM), Mineral |
|||
Linear Mold Shrinkage | 0.020 - 0.030 cm/cm @Thickness 3.20 mm |
0.020 - 0.030 in/in @Thickness 0.126 in |
ASTM D 955 |
RTP Company RTP 842 Acetal (POM); Mineral |
|||
Linear Mold Shrinkage | 0.020 - 0.023 cm/cm | 0.020 - 0.023 in/in | ASTM D955 |
PolyOne Lubri-Tech™ AT-000/20T Copolymer Acetal - 20% PTFE Lubricated
(discontinued **) Data provided by PolyOne. |
|||
Linear Mold Shrinkage | 0.020 - 0.025 cm/cm @Thickness 3.17 mm |
0.020 - 0.025 in/in @Thickness 0.125 in |
ASTM D955 |
PolyOne Lubri-Tech™ ATH-000/05M Acetal Homopolymer - 5% MoS2
(discontinued **) Data provided by PolyOne. |
|||
Linear Mold Shrinkage | 0.020 cm/cm | 0.020 in/in | ASTM D955 |
Kolon KOCETAL® DS500 Acid Resistant Acetal Resin Improved acid resistance. Applications: Products for improved chemical resistance. Information provided by API-Kolon. |
|||
Linear Mold Shrinkage | 0.020 cm/cm | 0.020 in/in | ASTM D955 |
Kolon Kocetal® K700 General Purpose Grade Acetal Copolymer Thermal properties: Kocetal has excellent heat stability; heat degradation is little under long term and high temperature application, compared to other POM. Maximum applicable temperature of produ.. |
|||
Linear Mold Shrinkage | 0.020 cm/cm | 0.020 in/in | ASTM D955 |
Kolon KOCETAL® MS301 Wear Modified Acetal Resin Molybdenum disulfide added, improved wear property. Applications: Products for low noise and friction against metal. Information provided by API-Kolon. |
|||
Linear Mold Shrinkage | 0.020 cm/cm | 0.020 in/in | ASTM D955 |
Kolon KOCETAL® WR301 Wear Modified Acetal Resin Improved weather resistant grade suitable for out door use. Applications: Weather resistant products. Information provided by API-Kolon. |
|||
Linear Mold Shrinkage | 0.020 cm/cm | 0.020 in/in | ASTM D955 |
Kolon KOCETAL® WR301LO Wear Modified Acetal Resin Improved weather resistance and low odor of FA. Applications: Weather resistant products at closed space. Information provided by API-Kolon. |
|||
Linear Mold Shrinkage | 0.020 cm/cm | 0.020 in/in | |
Momentive Performance Materials RTV12 Clear General Purpose Potting/Encapsulating Compound Two-part condensation cure. Two-part condensation cure silicones RTVs are designed to cute at room temperature, and can be applied at temperature up to one inch (2.5 cm). These are very tough mate.. |
|||
Linear Mold Shrinkage | 0.020 cm/cm | 0.020 in/in | After Curing |
Silikony Polskie Polastosil M-33 Silicone Rubber Medium hard with good tearing resistance |
|||
Linear Mold Shrinkage | 0.020 cm/cm | 0.020 in/in | After Curing |
Silikony Polskie Polastosil M-56 Silicone Rubber Rubber with strong hardness |
|||
Linear Mold Shrinkage | 0.020 cm/cm | 0.020 in/in | ASTM D955 |
Teknor Apex Monprene® MP-2327-R Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Linear Mold Shrinkage | 0.020 cm/cm | 0.020 in/in | |
Shin-Etsu Silicones LIMSâ„¢ KE1950-50A/B Elastomer KE-1950-50 is a liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. It's viscosity is low enough to allow easy .. |
|||
Linear Mold Shrinkage | 0.020 cm/cm @Thickness 3.17 mm |
0.020 in/in @Thickness 0.125 in |
ASTM D955 |
RTP Company RTP 1000 SI 2 Polybutylene Terephthalate (PBT), Silicone Lubricated |
|||
Linear Mold Shrinkage | 0.020 cm/cm @Thickness 3.17 mm |
0.020 in/in @Thickness 0.125 in |
ASTM D955 |
RTP Company RTP 1000 TFE 18 SI 2 Polybutylene Terephthalate (PBT), PTFE & Silicone Lubricated |
|||
Linear Mold Shrinkage | 0.020 - 0.040 cm/cm @Thickness 3.17 mm |
0.020 - 0.040 in/in @Thickness 0.125 in |
ASTM D955 |
RTP Company RTP 200 H TFE 20 SI 1 Impact-Modified Nylon 6/6 (PA), PTFE Lubricated - Silicone Lubricated |
|||
Linear Mold Shrinkage | 0.020 - 0.050 cm/cm | 0.020 - 0.050 in/in | |
Daikin POLYFLON MG-2030 PTFE 15% Graphite Filled Molding Powder 15% graphite filled. Low friction, excellent chemical resistance, high creep resistance.Applications: Mechanical and chemical service (e.g. bearings, gaskets, packings)Information provided by Daiki.. |
|||
Linear Mold Shrinkage | 0.020 cm/cm | 0.020 in/in | ASTM D955 |
Clariant Renol PA133GN-109 Nylon 66, High Impact, Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Linear Mold Shrinkage | 0.020 - 0.050 cm/cm | 0.020 - 0.050 in/in | |
Daikin POLYFLON MG-1030F PTFE 15% Glass Fiber Filled Molding Powder, High Apparent Density, Free Flow 15% glass fiber filled. High apparent density and free-flowing properties. High wear resistance, low friction, good electrical properties.Applications: Mechanical and electrical service. Availabl.. |
|||
Linear Mold Shrinkage | 0.020 cm/cm | 0.020 in/in | ASTM D955 |
Aclo Accucomp Polyacetal (POM) ACE092L Medium Viscosity |
|||
Linear Mold Shrinkage | 0.020 cm/cm | 0.020 in/in | ASTM Data; MD |
BASF Ultraform N 2320 U03 UNC Q600 POM Ultraform N2320 U03 UNC Q600 is a rapidly freezing UV stabilized general-purpose injection molding grade. |
|||
Linear Mold Shrinkage | 0.020 cm/cm @Thickness 2.00 mm |
0.020 in/in @Thickness 0.0787 in |
ISO 294-4 |
Ascend Performance Materials Vydyne® 21SPF Nylon 66, General Purpose, High Productivity, Conditioned Vydyne® 21SPF is general-purpose PA66 resin. Available in natural, it is designed principally for injection-molding fabrication. This grade offers a well-balanced combination of engineering propert.. |
|||
Linear Mold Shrinkage | 0.020 cm/cm | 0.020 in/in | |
3M Dyneon™ PVDF 6108/0001 Polyvinylidene Fluoride Polyvinylidene Fluoride (PVDF) is ideal for multiple applications across a wide array of industries. Widely used in the chemical process industry, wire and cable industry, semiconductor industry, an.. |
|||
Linear Mold Shrinkage | 0.020 - 0.030 cm/cm | 0.020 - 0.030 in/in | |
Solvay Specialty Polymers Solef® 1010 PVDF Homopolymer
(discontinued **) Key features of this grade: Med Viscosity, All Purpose, Extrusion, Virgin. Recommended processing is extrusion. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® PVDF .. |
|||
Linear Mold Shrinkage | 0.020 cm/cm | 0.020 in/in | ASTM D955 |
PolyOne Synprene® ST-6250 Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:Over-Molding GradeUV StabilizedApplications:Multi-PurposeProcessing Method:Injection MoldingPolyOne First ChoiceInformation provided by PolyOne Corporation. |