Polymer Property : Linear Mold Shrinkage = 0.0120 cm/cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.00800 - 0.0120 cm/cm
0.00800 - 0.0120 in/in
ASTM D955
Niche Polymer PA66GM40BK Nylon 66, 40% Mineral Fiber Filled
Information provided by Niche Polymer
Linear Mold Shrinkage 0.00800 - 0.0120 cm/cm
0.00800 - 0.0120 in/in
ASTM D955
Niche Polymer PA66GM40N Nylon 66, 40% Mineral Fiber Filled
Information provided by Niche Polymer
Linear Mold Shrinkage 0.00800 - 0.0120 cm/cm
0.00800 - 0.0120 in/in
ASTM D955
Niche Polymer PPCT20BK Copolymer PP, 20% Talc Filled
Information provided by Niche Polymer
Linear Mold Shrinkage 0.00200 - 0.0120 cm/cm
0.00200 - 0.0120 in/in
Average value: 0.00618 cm/cm Grade Count:216
Overview of materials for Polycarbonate, Unreinforced, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Unreinforced, Flame Retardant". Each property range of values reported is minimum and max..
Linear Mold Shrinkage 0.00100 - 0.0120 cm/cm
0.00100 - 0.0120 in/in
Average value: 0.00503 cm/cm Grade Count:19
Overview of materials for Polycarbonate, Conductive
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Conductive". Each property range of values reported is minimum and maximum values of appr..
Linear Mold Shrinkage 0.00500 - 0.0120 cm/cm
0.00500 - 0.0120 in/in
Average value: 0.00800 cm/cm Grade Count:7
Overview of materials for Polycarbonate/Thermoplastic Polyurethane Blend
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Thermoplastic Polyurethane Blend". Each property range of values reported is minimum and m..
Linear Mold Shrinkage 0.000500 - 0.0120 cm/cm
0.000500 - 0.0120 in/in
Average value: 0.00394 cm/cm Grade Count:76
Overview of materials for PVC, Rigid Grade
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Rigid Grade". Each property range of values reported is minimum and maximum values of appropriate M..
Linear Mold Shrinkage 0.000900 - 0.0120 cm/cm
0.000900 - 0.0120 in/in
Average value: 0.00745 cm/cm Grade Count:41
Overview of materials for Polypropylene with 20% Mica Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Mica Filler". Specific grades with primary filler content between 15% and 24% are..
Linear Mold Shrinkage 0.00830 - 0.0120 cm/cm
0.00830 - 0.0120 in/in
Average value: 0.00953 cm/cm Grade Count:3
Overview of materials for Thermoplastic Polyimide, Unfilled
Linear Mold Shrinkage 0.00330 - 0.0120 cm/cm
0.00330 - 0.0120 in/in
Average value: 0.00687 cm/cm Grade Count:12
Overview of materials for Phenolic, Novolac, Heat Resistant Grade, Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Heat Resistant Grade, Filled". Each property range of values reported is minimum and ..
Linear Mold Shrinkage 0.00350 - 0.0120 cm/cm
0.00350 - 0.0120 in/in
Average value: 0.00708 cm/cm Grade Count:21
Overview of materials for Phenolic, Novolac, Impact Grade, Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Impact Grade, Filled". Each property range of values reported is minimum and maximum ..
Linear Mold Shrinkage 0.00200 - 0.0120 cm/cm
0.00200 - 0.0120 in/in
Average value: 0.00833 cm/cm Grade Count:10
Overview of materials for Nylon 6, Mineral Reinforced, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Mineral Reinforced, Impact Grade". Each property range of values reported is minimum and maximu..
Linear Mold Shrinkage 0.00100 - 0.0120 cm/cm
0.00100 - 0.0120 in/in
Average value: 0.00366 cm/cm Grade Count:16
Overview of materials for Nylon 12, 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 20% Glass Fiber Filled". Specific grades with glass content between 15% and 24% are included. ..
Linear Mold Shrinkage 0.000 - 0.0120 cm/cm
0.000 - 0.0120 in/in
Average value: 0.00205 cm/cm Grade Count:38
Overview of materials for Polycarbonate, 40% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 40% Glass Filled". Specific grades with glass content between 35% and 44% are included. E..
Linear Mold Shrinkage 0.00200 - 0.0120 cm/cm
0.00200 - 0.0120 in/in
Average value: 0.00509 cm/cm Grade Count:21
Overview of materials for Polybutylene Terephthalate (PBT), Glass Fiber + PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Fiber + PTFE Filled". Each property range of values reported is ..
Linear Mold Shrinkage 0.00150 - 0.0120 cm/cm
0.00150 - 0.0120 in/in
Average value: 0.00433 cm/cm Grade Count:33
Overview of materials for Polyethylene Terephthalate (PET), 20% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 20% Glass Reinforced". Specific grades with glass content between 15% ..
Linear Mold Shrinkage 0.000500 - 0.0120 cm/cm
0.000500 - 0.0120 in/in
Average value: 0.00377 cm/cm Grade Count:24
Overview of materials for Polyphthalamide (PPA), Glass/PTFE
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide + Glass/PTFE". Each property range of values reported is minimum and maximum values of a..