Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Overview of materials for Polycarbonate/Thermoplastic Polyurethane Blend

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate/Thermoplastic Polyurethane Blend , Polyurethane, TP
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Overview of materials for Polycarbonate/Thermoplastic Polyurethane Blend.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Thermoplastic Polyurethane Blend". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.15 - 1.18 g/cc
0.0415 - 0.0426 lb/in³
Average value: 1.15 g/cc Grade Count:7
Linear Mold Shrinkage 0.00500 - 0.0120 cm/cm
0.00500 - 0.0120 in/in
Average value: 0.00800 cm/cm Grade Count:7
Mechanical Properties Metric English Comments
Hardness, Shore A 73.0 - 95.0
73.0 - 95.0
Average value: 84.0 Grade Count:3
Tensile Strength, Ultimate 36.5 - 55.2 MPa
5300 - 8000 psi
Average value: 48.1 MPa Grade Count:7
Tensile Strength, Yield 2.07 - 53.8 MPa
300 - 7800 psi
Average value: 18.4 MPa Grade Count:7
Elongation at Break 370 - 470 %
370 - 470 %
Average value: 400 % Grade Count:5
Flexural Modulus 0.00427 - 2.62 GPa
0.620 - 380 ksi
Average value: 0.743 GPa Grade Count:7