Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.00500 cm/cm | 0.00500 in/in | ASTM D955 |
Niche Polymer PPHG20BK Homopolymer PP, 20% Glass Fiber Filled Information provided by Niche Polymer |
|||
Linear Mold Shrinkage | 0.00500 - 0.0160 cm/cm | 0.00500 - 0.0160 in/in | Average value: 0.00715 cm/cm Grade Count:53 |
Overview of materials for Polyphenylene Ether, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Molded". Each property range of values reported is minimum and maximum values of ap.. |
|||
Linear Mold Shrinkage | 0.00500 - 0.00700 cm/cm | 0.00500 - 0.00700 in/in | Average value: 0.00600 cm/cm Grade Count:8 |
Overview of materials for Polyphenylene Ether, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Impact Grade". Each property range of values reported is minimum and maximum values.. |
|||
Linear Mold Shrinkage | 0.00500 - 0.0300 cm/cm | 0.00500 - 0.0300 in/in | Average value: 0.0112 cm/cm Grade Count:34 |
Overview of materials for Acetal Copolymer, 10% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% ar.. |
|||
Linear Mold Shrinkage | 0.00500 - 0.0300 cm/cm | 0.00500 - 0.0300 in/in | Average value: 0.0160 cm/cm Grade Count:29 |
Overview of materials for Acetal Copolymer, Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Mineral Filled". Each property range of values reported is minimum and maximum values .. |
|||
Linear Mold Shrinkage | 0.00500 - 0.00800 cm/cm | 0.00500 - 0.00800 in/in | Average value: 0.00628 cm/cm Grade Count:15 |
Overview of materials for Polycarbonate, Gamma Radiation Resistant This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Gamma Radiation Resistant". Each property range of values reported is minimum and maximum.. |
|||
Linear Mold Shrinkage | 0.00500 - 0.0120 cm/cm | 0.00500 - 0.0120 in/in | Average value: 0.00800 cm/cm Grade Count:7 |
Overview of materials for Polycarbonate/Thermoplastic Polyurethane Blend This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Thermoplastic Polyurethane Blend". Each property range of values reported is minimum and m.. |
|||
Linear Mold Shrinkage | 0.00500 - 0.0200 cm/cm | 0.00500 - 0.0200 in/in | Average value: 0.0124 cm/cm Grade Count:7 |
Overview of materials for Nylon 66, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Extruded". Each property range of values reported is minimum and maximum values of appropriate.. |
|||
Linear Mold Shrinkage | 0.00500 - 0.0220 cm/cm | 0.00500 - 0.0220 in/in | Average value: 0.0111 cm/cm Grade Count:15 |
Overview of materials for Nylon 66, Mineral Filled, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Mineral Filled, Impact Grade". Each property range of values reported is minimum and maximum v.. |
|||
Linear Mold Shrinkage | 0.00500 - 0.00800 cm/cm | 0.00500 - 0.00800 in/in | Average value: 0.00675 cm/cm Grade Count:4 |
Overview of materials for High Density Polyethylene (HDPE), Extruded This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Extruded". Each property range of values reported is minimum and maxim.. |
|||
Linear Mold Shrinkage | 0.00500 - 0.0100 cm/cm | 0.00500 - 0.0100 in/in | Average value: 0.00833 cm/cm Grade Count:3 |
Overview of materials for PEKK, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "PEKK, Unreinforced". Each property range of values reported is minimum and maximum values of appropriate.. |
|||
Linear Mold Shrinkage | 0.00500 - 0.0450 cm/cm | 0.00500 - 0.0450 in/in | Average value: 0.0123 cm/cm Grade Count:15 |
Overview of materials for Thermoplastic Polyurethane (TPUR), Polyether Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Polyether Grade". Each property range of values reported is minimum a.. |
|||
Linear Mold Shrinkage | 0.00500 - 0.00500 cm/cm @Temperature 80.0 - 80.0 °C |
0.00500 - 0.00500 in/in @Temperature 176 - 176 °F |
Average value: 0.00500 cm/cm Grade Count:1 |
Overview of materials for Nylon 6, 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. .. |