Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.00800 - 0.0120 cm/cm | 0.00800 - 0.0120 in/in | ASTM D955 |
Niche Polymer PA66GM40BK Nylon 66, 40% Mineral Fiber Filled Information provided by Niche Polymer |
|||
Linear Mold Shrinkage | 0.00800 - 0.0120 cm/cm | 0.00800 - 0.0120 in/in | ASTM D955 |
Niche Polymer PA66GM40N Nylon 66, 40% Mineral Fiber Filled Information provided by Niche Polymer |
|||
Linear Mold Shrinkage | 0.00800 - 0.0120 cm/cm | 0.00800 - 0.0120 in/in | ASTM D955 |
Niche Polymer PPCT20BK Copolymer PP, 20% Talc Filled Information provided by Niche Polymer |
|||
Linear Mold Shrinkage | 0.00800 cm/cm | 0.00800 in/in | ASTM D955 |
Niche Polymer PPHT40BK Homopolymer PP, 40% Talc Fiber Filled Information provided by Niche Polymer |
|||
Linear Mold Shrinkage | 0.00800 - 0.0300 cm/cm | 0.00800 - 0.0300 in/in | Average value: 0.0164 cm/cm Grade Count:29 |
Overview of materials for Acetal Copolymer, Aramid Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Aramid Fiber Filled". Each property range of values reported is minimum and maximum va.. |
|||
Linear Mold Shrinkage | 0.00800 - 0.0110 cm/cm @Temperature 121 - 121 °C |
0.00800 - 0.0110 in/in @Temperature 250 - 250 °F |
Average value: 0.00950 cm/cm Grade Count:1 |
Overview of materials for Polypropylene, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Molded". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Linear Mold Shrinkage | 0.00800 - 0.0110 cm/cm @Time 1800 - 1800 sec |
0.00800 - 0.0110 in/in @Time 0.500 - 0.500 hour |
Average value: 0.00950 cm/cm Grade Count:1 |
Overview of materials for Polypropylene, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Molded". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Linear Mold Shrinkage | 0.00800 - 0.0250 cm/cm | 0.00800 - 0.0250 in/in | Average value: 0.0131 cm/cm Grade Count:11 |
Overview of materials for Nylon 612, Aramid Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Aramid Fiber Filled". Each property range of values reported is minimum and maximum values of.. |
|||
Linear Mold Shrinkage | 0.00800 - 0.0400 cm/cm | 0.00800 - 0.0400 in/in | Average value: 0.0192 cm/cm Grade Count:26 |
Overview of materials for High Density Polyethylene (HDPE), Injection Molded This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Injection Molded". Each property range of values reported is minimum a.. |
|||
Linear Mold Shrinkage | 0.00800 - 0.0226 cm/cm | 0.00800 - 0.0226 in/in | Average value: 0.0143 cm/cm Grade Count:26 |
Overview of materials for Polypropylene Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene Glass Bead Filled". Each property range of values reported is minimum and maximum values o.. |
|||
Linear Mold Shrinkage | 0.00800 - 0.0350 cm/cm | 0.00800 - 0.0350 in/in | Average value: 0.0193 cm/cm Grade Count:33 |
Overview of materials for Acetal Copolymer, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Impact Modified". Each property range of values reported is minimum and maximum values.. |
|||
Linear Mold Shrinkage | 0.00800 - 0.0160 cm/cm | 0.00800 - 0.0160 in/in | Average value: 0.0109 cm/cm Grade Count:14 |
Overview of materials for Polypropylene with 10% Mica Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Mica Filler". Specific grades with primary filler content between 5% and 14% are .. |
|||
Linear Mold Shrinkage | 0.00800 - 0.0190 cm/cm | 0.00800 - 0.0190 in/in | Average value: 0.0141 cm/cm Grade Count:35 |
Overview of materials for Polypropylene with 10% Calcium Carbonate (CaCO3) Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Calcium Carbonate (CaCO3) Filler". Specific grades with primary filler content be.. |