Polymer Property : Linear Mold Shrinkage = 0.00830 cm/cm
Polymer Property :
Linear Mold Shrinkage =
0.00830 cm/cm
Product List
Physical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties
Metric
English
Comments
Linear Mold Shrinkage
0.00830
-
0.0120
cm/cm
0.00830
-
0.0120
in/in
Average value: 0.00953 cm/cm Grade Count:3
Overview of materials for Thermoplastic Polyimide, Unfilled